ASTM A270 Grade TP316 Hot Finished or Cold Finished
Equivalent material: AISI 316, SAE 316, JIS SUS316, UNS S31600, DIN 1.4984, AFNOR 9165-041, AFNOR 9165 25, AFNOR Z 10 CNW 17, EN 1.4984, ASTM 316, ASTM F316, ASTM S31600, ASTM B8M
ASTM A270 Grade TP316 Hot Finished or Cold Finished general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.9 - 8.2 g/cm³ |
Typical for Austenitic Stainless Steel |
ASTM A270 Grade TP316 Hot Finished or Cold Finished thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K |
Typical for Austenitic Stainless Steel |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 J/(kg·K) |
Typical for Austenitic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
ASTM A270 Grade TP316 Hot Finished or Cold Finished electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
ASTM A270 Grade TP316 Hot Finished or Cold Finished mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 195 GPa |
Typical for Austenitic Stainless Steel |
Elongation A50 |
23.0 °C |
Elongation A50 of 35 % |
- |
Hardness, Rockwell B |
23.0 °C |
Hardness, Rockwell B of 90 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 515 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 205 MPa |
- |