Amstrong® 500MC Laser

Amstrong® 500MC Laser introduction

The Amstrong® Laser sheet range comprises hot rolled steel grades developed for applications using computer-controlled thermal and mechanical cutting equipment (laser, plasma etc). The sheets are cut to length from ArcelorMittal coils for laser applications on certified lines that are able to reduce internal stresses and improve flatness before, during and after cutting.


All these grades are designed to:

Give improved productivity, quality and consistency with laser cutting

Meet the most stringent flatness requirements after cutting
Amstrong® Laser sheets are virtually free of internal stresses and can therefore be used to produce sheets with guaranteed flatness before, during and after cutting.

Equivalent material: EN S500MC

Amstrong® 500MC Laser general

Property Value Comment
Carbon equivalent (CEV) Carbon equivalent (CEV) of 0.42 [-] max.

Amstrong® 500MC Laser chemical

Property Value Comment
Aluminium Aluminium of 0.015 % min.
Carbon Carbon of 0.12 % max.
Manganese Manganese of 1.7 % max.
Niobium Niobium of 0.09 % max.
Phosphorus Phosphorus of 0.02 % max.
Silicon Silicon of 0.03 % max.
Sulfur Sulfur of 0.012 % max.
Titanium Titanium of 0.15 % max.
Vanadium Vanadium of 0.2 % max.

Amstrong® 500MC Laser electrical

Property - -
Application areas
Chemical composition
Delivery condtion
Other - Laser Classic Laser Premium Side trimmed* -
For sheets Maximum deviation: the minimum value, depending on the circumstances, between 4 mm/m or 8 mm/2 m or 12 mm/3 m and the special tolerances in EN 10051:2010 Maximum deviation: the minimum value, depending on the circumstances, between 3 mm/m or 6 mm/2 m or 9 mm/3 m and the special tolerances in EN 10051:2010 Min width Max width
On cut parts Maximum deviation of 5 mm over a length of 1 m Maximum deviation of 3 mm over a length of 1 m 595 1640

Amstrong® 500MC Laser mechanical

Property Temperature Value Comment
Charpy impact energy -20 °C Charpy impact energy of 40 J min. | for thickness 6-16 mm
Elongation - Elongation of 14 % min. | for thickness < 2 mm | Transverse, A80
- - Elongation of 15 % min. | for thickness < 2 mm, A80
- - Elongation of 15 % min. | for thickness 2-3 mm | Transverse, A80
- - Elongation of 16 % min. | for thickness 2-3 mm, A80
- - Elongation of 18 % min. A5.65√So | for thickness 3-16 mm | Transverse
- - Elongation of 19 % min. A5.65√So | for thickness 3-16 mm
Tensile strength - Tensile strength of 560 - 700 MPa for thickness < 16 mm
- - Tensile strength of 570 - 700 MPa for thickness < 16 mm | Transverse
Yield strength - Yield strength of 500 - 600 MPa for thickness < 16 mm
- - Yield strength of 530 - 630 MPa for thickness < 16 mm | Transverse