Property Temperature Value
Density 23.0 °C Density of 7.9 g/cm³

AISI 4320 Normalized thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.2E-5 1/K -
Melting point - Melting point of 1382 - 1529 °C Typical for Nickel Chromium Molybdenum Steel
Specific heat capacity 23.0 °C Specific heat capacity of 450 J/(kg·K) -
Thermal conductivity 23.0 °C Thermal conductivity of 34 - 54 W/(m·K) Typical for Nickel Chromium Molybdenum Steel

AISI 4320 Normalized chemical

Property Value
Carbon Carbon of 0.17 - 0.22 %
Chromium Chromium of 0.4 - 0.6 %
Iron Iron of 95.8 - 97 %
Manganese Manganese of 0.45 - 0.65 %
Molybdenum Molybdenum of 0.2 - 0.3 %
Nickel Nickel of 1.7 - 2 %
Phosphorus Phosphorus of 0 - 0.04 %
Silicon Silicon of 0.15 - 0.35 %
Sulfur Sulfur of 0 - 0.04 %

AISI 4320 Normalized mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 210 GPa -
Elongation 23.0 °C Elongation of 21 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Nickel Chromium Molybdenum Steel
Tensile strength 23.0 °C Tensile strength of 790 MPa -
Yield strength 23.0 °C Yield strength of 460 MPa -