AISI 1037 Hot Rolled
Equivalent material: DIN 1.0561, SAE 1037, EN 1.0561, ASTM 1037, UNS G10370
AISI 1037 Hot Rolled general
Property |
Temperature |
Value |
Density |
23.0 °C |
Density of 7.8 g/cm³ |
AISI 1037 Hot Rolled thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.2E-5 1/K |
- |
Max service temperature |
- |
Max service temperature of 500 °C |
Typical for Carbon Steel |
Melting point |
- |
Melting point of 1380 - 1514 °C |
Typical for Medium Carbon Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 450 J/(kg·K) |
- |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 21 - 52 W/(m·K) |
Typical for Medium Carbon Steel |
AISI 1037 Hot Rolled chemical
Property |
Value |
Carbon |
Carbon of 0.32 - 0.38 % |
Iron |
Iron of 98.5 - 99 % |
Manganese |
Manganese of 0.7 - 1 % |
Phosphorus |
Phosphorus of 0 - 0.04 % |
Sulfur |
Sulfur of 0 - 0.05 % |
AISI 1037 Hot Rolled electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m |
Typical for Carbon Steel |
AISI 1037 Hot Rolled mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 210 GPa |
- |
Elongation |
23.0 °C |
Elongation of 21 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Medium Carbon Steel |
Shear modulus |
23.0 °C |
Shear modulus of 75 - 80 GPa |
Typical for Carbon Steel |
Tensile strength |
23.0 °C |
Tensile strength of 590 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 320 MPa |
- |