UNS S32654 Solution Treated
Equivalent material: DIN 1.4652, AISI S32654, SAE S32654, EN X1CrNiMoCuN24-22-8, EN 1.4652, ASTM S32654
UNS S32654 Solution Treated general
Property |
Temperature |
Value |
Density |
23.0 °C |
Density of 8.1 g/cm³ |
UNS S32654 Solution Treated thermal
Property |
Temperature |
Value |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.3E-5 1/K |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 500 J/(kg·K) |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 8.6 W/(m·K) |
UNS S32654 Solution Treated chemical
Property |
Value |
Carbon |
Carbon of 0 - 0.02 % |
Chromium |
Chromium of 23 - 25 % |
Copper |
Copper of 0.3 - 0.6 % |
Iron |
Iron of 38.3 - 46.3 % |
Manganese |
Manganese of 2 - 4 % |
Molybdenum |
Molybdenum of 7 - 8 % |
Nickel |
Nickel of 21 - 23 % |
Nitrogen |
Nitrogen of 0.45 - 0.55 % |
Phosphorus |
Phosphorus of 0 - 0.03 % |
Silicon |
Silicon of 0 - 0.5 % |
Sulfur |
Sulfur of 0 - 5E-3 % |
UNS S32654 Solution Treated mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 190 GPa |
- |
Elongation |
23.0 °C |
Elongation of 46 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Steel |
Tensile strength |
23.0 °C |
Tensile strength of 880 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 490 MPa |
- |