UNS S15700 Annealed
Equivalent material: DIN 1.4532, EN X8CrNiMoAl15-7-2, EN 1.4532, DIN 1.4574, AFNOR 9160/C65, AFNOR 9160C211, AFNOR Z6CND15-07, AISI PH15-7-Mo, AISI 632 (15-7PH), SAE PH15-7-Mo, SAE 632 (15-7PH), EN FE-PM 63, EN 1.4574, ASTM 632
UNS S15700 Annealed general
Property |
Temperature |
Value |
Density |
23.0 °C |
Density of 7.8 g/cm³ |
UNS S15700 Annealed thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.3E-5 1/K |
- |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 450 J/(kg·K) |
- |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
UNS S15700 Annealed chemical
Property |
Value |
Aluminium |
Aluminium of 0.75 - 1.5 % |
Carbon |
Carbon of 0 - 0.09 % |
Chromium |
Chromium of 14 - 16 % |
Iron |
Iron of 69.6 - 76.8 % |
Manganese |
Manganese of 0 - 1 % |
Molybdenum |
Molybdenum of 2 - 3 % |
Nickel |
Nickel of 6.5 - 7.7 % |
Phosphorus |
Phosphorus of 0 - 0.04 % |
Silicon |
Silicon of 0 - 1 % |
Sulfur |
Sulfur of 0 - 0.03 % |
UNS S15700 Annealed electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
UNS S15700 Annealed mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 220 GPa |
- |
Elongation |
23.0 °C |
Elongation of 29 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 1190 MPa |
- |
Yield strength |
23.0 °C |
Yield strength of 520 MPa |
- |