SAE J775 Grade NV-5
Equivalent material: AISI NV-5, SAE NV-5, UNS G86450
SAE J775 Grade NV-5 general
Property |
Temperature |
Value |
Comment |
Density |
20.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Nickel Chromium Molybdenum Steel |
SAE J775 Grade NV-5 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
500.0 °C |
Coefficient of thermal expansion of 1.35E-5 1/K |
The mentioned value is between 20°C and the mentioned temperature |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Nickel Chromium Molybdenum Steel |
Thermal conductivity |
20.0 °C |
Thermal conductivity of 34 - 54 W/(m·K) |
Typical for Nickel Chromium Molybdenum Steel |
SAE J775 Grade NV-5 chemical
Property |
Value |
Carbon |
Carbon of 0.43 - 0.48 % |
Chromium |
Chromium of 0.4 - 0.6 % |
Iron |
Balance |
Manganese |
Manganese of 0.75 - 1 % |
Molybdenum |
Molybdenum of 0.25 - 1.5 % |
Nickel |
Nickel of 0.4 - 0.7 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 0.15 - 0.35 % |
Sulfur |
Sulfur of 0.04 % |
SAE J775 Grade NV-5 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
20.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Nickel Chromium Molybdenum Steel |
Hardness, Rockwell C |
20.0 °C |
Hardness, Rockwell C of 35 [-] |
- |
Poisson's ratio |
20.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Nickel Chromium Molybdenum Steel |
Reduction of area |
20.0 °C |
Reduction of area of 40 % |
- |
Tensile strength |
20.0 °C |
Tensile strength of 1240 MPa |
- |
Yield strength |
20.0 °C |
Yield strength of 1140 MPa |
- |