SAE J775 Grade XEV-D
SAE J775 Grade XEV-D general
| Property | Temperature | Value |
|---|---|---|
| Reduction of area | 20.0 °C | Reduction of area of 66 % |
| - | 760.0 °C | Reduction of area of 31 % |
| Tensile strength | 20.0 °C | Tensile strength of 800 MPa |
| - | 760.0 °C | Tensile strength of 320 MPa |
| Yield strength | 20.0 °C | Yield strength of 360 MPa |
| - | 760.0 °C | Yield strength of 170 MPa |
SAE J775 Grade XEV-D chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.55 % |
| Chromium | Chromium of 21 % |
| Iron | Iron of 64.7 - 100 % |
| Manganese | Manganese of 8.25 % |
| Nickel | Nickel of 2.8 % |
| Nitrogen | Nitrogen of 0.45 % |
| Silicon | Silicon of 0.15 % |
| Tungsten | Tungsten of 1.75 % |
| Vanadium | Vanadium of 0.35 % |