SAE J405 Grade S32803
Equivalent material: DIN 1.4475, DIN X1CrNiMoNb28-4-2, AISI S32803, EN 1.4475, GB/T S12871, GB/T 012Cr28Ni4Mo2Nb, ASTM S32803, UNS S32803
SAE J405 Grade S32803 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.6 - 7.8 g/cm³ |
Typical for Ferritic Stainless Steel |
SAE J405 Grade S32803 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 9.3E-6 - 1.2E-5 1/K |
Typical for Ferritic Stainless Steel |
Melting point |
- |
Melting point of 1425 - 1530 °C |
Typical for Ferritic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 420 - 586 J/(kg·K) |
Typical for Ferritic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 22 W/(m·K) |
Typical for Ferritic Stainless Steel |
SAE J405 Grade S32803 chemical
Property |
Value |
Carbon |
Carbon of 0.015 % |
Chromium |
Chromium of 28 - 29 % |
Manganese |
Manganese of 0.5 % |
Molybdenum |
Molybdenum of 1.8 - 2.5 % |
Nickel |
Nickel of 3 - 4 % |
Niobium |
Niobium of 0.15 - 0.5 % |
Nitrogen |
Nitrogen of 0.02 % |
Phosphorus |
Phosphorus of 0.02 % |
Silicon |
Silicon of 0.55 % |
Sulfur |
Sulfur of 3.5E-3 % |
SAE J405 Grade S32803 electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 6E-7 - 7.5E-7 Ω·m |
Typical for Ferritic Stainless Steel |
SAE J405 Grade S32803 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 220 GPa |
Typical for Ferritic Stainless Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Ferritic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Ferritic Stainless Steel |