SAE J405 Grade 317LN
Equivalent material: DIN 1.4434, AISI 317LN, JIS SUS317LN, EN X2CrNiMoN18-12-4, EN 1.4434, ASTM 317LN, UNS S31753
SAE J405 Grade 317LN general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.9 - 8.2 g/cm³ |
Typical for Austenitic Stainless Steel |
SAE J405 Grade 317LN thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K |
Typical for Austenitic Stainless Steel |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 J/(kg·K) |
Typical for Austenitic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
SAE J405 Grade 317LN chemical
Property |
Value |
Carbon |
Carbon of 0.03 % |
Chromium |
Chromium of 18 - 20 % |
Manganese |
Manganese of 2 % |
Molybdenum |
Molybdenum of 3 - 4 % |
Nickel |
Nickel of 11 - 15 % |
Nitrogen |
Nitrogen of 0.1 - 0.22 % |
Phosphorus |
Phosphorus of 0.05 % |
Silicon |
Silicon of 0.75 % |
Sulfur |
Sulfur of 0.03 % |
SAE J405 Grade 317LN electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
SAE J405 Grade 317LN mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 195 GPa |
Typical for Austenitic Stainless Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |