SAE J405 Grade 201
Equivalent material: DIN 1.4372, DIN X12CrMnNiN17-7-5, AISI 201, JIS SUS201, EN X12CrMnNiN17-7-5, EN 1.4372, ISO X12CrMnNiN17-7-5, ISO 4372-201-00-I, ISO AP29O, ISO 13, ASTM TP201, ASTM 201-1, ASTM 201-2, UNS S20100, ASTM 201
SAE J405 Grade 201 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.9 - 8.2 g/cm³ |
Typical for Austenitic Stainless Steel |
SAE J405 Grade 201 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K |
Typical for Austenitic Stainless Steel |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 J/(kg·K) |
Typical for Austenitic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
SAE J405 Grade 201 chemical
Property |
Value |
Carbon |
Carbon of 0.15 % |
Chromium |
Chromium of 16 - 18 % |
Manganese |
Manganese of 5.5 - 7.5 % |
Nickel |
Nickel of 3.5 - 5.5 % |
Nitrogen |
Nitrogen of 0.25 % |
Phosphorus |
Phosphorus of 0.06 % |
Silicon |
Silicon of 1 % |
Sulfur |
Sulfur of 0.03 % |
SAE J405 Grade 201 electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
SAE J405 Grade 201 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 195 GPa |
Typical for Austenitic Stainless Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |