SAE J403 Grade 1085
Equivalent material: DIN 1.1273, DIN 90Mn4, AISI 1085, JIS SWRH87, EN 1.1273, UNS G10850
SAE J403 Grade 1085 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for High Carbon Steel |
SAE J403 Grade 1085 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.32E-5 1/K |
Typical for High Carbon Steel |
Max service temperature |
- |
Max service temperature of 500 °C |
Typical for Carbon Steel |
Melting point |
- |
Melting point of 1289 - 1478 °C |
Typical for High Carbon Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 486 J/(kg·K) |
Typical for High Carbon Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 36 W/(m·K) |
Typical for High Carbon Steel |
SAE J403 Grade 1085 chemical
Property |
Value |
Aluminium |
Aluminium of 0.02 % |
Carbon |
Carbon of 0.8 - 0.93 % |
Chromium |
Chromium of 0.02 % |
Copper |
Copper of 0.02 % |
Iron |
balance |
Manganese |
Manganese of 0.7 - 1 % |
Molybdenum |
Molybdenum of 0.02 % |
Nickel |
Nickel of 0.02 % |
Niobium |
Niobium of 0.08 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 0.02 % |
Sulfur |
Sulfur of 0.035 % |
Titanium |
Titanium of 0.08 % |
Vanadium |
Vanadium of 0.08 % |
SAE J403 Grade 1085 electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m |
Typical for Carbon Steel |
SAE J403 Grade 1085 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for High Carbon Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for High Carbon Steel |
Shear modulus |
23.0 °C |
Shear modulus of 81 GPa |
Typical for High Carbon Steel |