SAE J1392 Grade 070YL hot-rolled

Equivalent material: AISI 070ZL, AISI 070YL, SAE 070ZL

SAE J1392 Grade 070YL hot-rolled general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Low Carbon Steel

SAE J1392 Grade 070YL hot-rolled thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K Typical for Low Carbon Steel
Max service temperature - Max service temperature of 500 °C Typical for Carbon Steel
Melting point - Melting point of 1480 - 1526 °C Typical for Low Carbon Steel
Specific heat capacity 23.0 °C Specific heat capacity of 465 J/(kg·K) Typical for Low Carbon Steel
Thermal conductivity 23.0 °C Thermal conductivity of 25 - 93 W/(m·K) Typical for Low Carbon Steel

SAE J1392 Grade 070YL hot-rolled chemical

Property Value Comment
Iron Iron of 98.35 - 100 % balance
Manganese Manganese of 1.65 % -

SAE J1392 Grade 070YL hot-rolled magnetic

Property Value Comment
Curie temperature Curie temperature of 770 °C Typical for Low Carbon Steel

SAE J1392 Grade 070YL hot-rolled electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m Typical for Carbon Steel

SAE J1392 Grade 070YL hot-rolled mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Low Carbon Steel
Elongation 23.0 °C Elongation of 17 % -
Elongation A50 23.0 °C Elongation A50 of 17 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Low Carbon Steel
Shear modulus 23.0 °C Shear modulus of 82 GPa Typical for Low Carbon Steel
Tensile strength 23.0 °C Tensile strength of 590 MPa -
Yield strength 23.0 °C Yield strength of 480 MPa -