SAE J1268 Grade 8660H
Equivalent material: DIN 1.6528, DIN GS60NiCrMo2, AISI 8660H, EN 1.6528, UNS H86600
SAE J1268 Grade 8660H general
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
SAE J1268 Grade 8660H thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
| Melting point | - | Melting point of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel |
| Specific heat capacity | 23.0 °C | Specific heat capacity of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
| Thermal conductivity | 23.0 °C | Thermal conductivity of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |
SAE J1268 Grade 8660H chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.55 - 0.65 % |
| Chromium | Chromium of 0.35 - 0.65 % |
| Copper | Copper of 0.35 % |
| Iron | balance |
| Manganese | Manganese of 0.7 - 1.05 % |
| Molybdenum | Molybdenum of 0.15 - 0.25 % |
| Nickel | Nickel of 0.35 - 0.75 % |
| Phosphorus | Phosphorus of 0.03 % |
| Silicon | Silicon of 0.15 - 0.35 % |
| Sulfur | Sulfur of 0.04 % |
SAE J1268 Grade 8660H mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
| Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Choose our top-grade steel products for unparalleled strength and unwavering quality.
-- Our promise