JIS H45521 Grade NCuT annealed

Equivalent material: JIS NCuP-O, AMS 4674D, ASTM N04405

JIS H45521 Grade NCuT annealed general

Property Temperature Value Comment
Density 23.0 °C Density of 8.8 g/cm³ Typical for Nickel Steel

JIS H45521 Grade NCuT annealed thermal

Property Temperature Value Comment
Melting point - Melting point of 1316 - 1595 °C Typical for Nickel Steel
Specific heat capacity 23.0 °C Specific heat capacity of 456 J/(kg·K) Typical for Nickel Steel
Thermal conductivity 23.0 °C Thermal conductivity of 10 - 50 W/(m·K) Typical for Nickel Steel

JIS H45521 Grade NCuT annealed mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Nickel Steel
Elongation 23.0 °C Elongation of 35 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Nickel Steel
Shear modulus 23.0 °C Shear modulus of 76 GPa Typical for Nickel Steel
Tensile strength 23.0 °C Tensile strength of 481 MPa -