JIS H4501 Grade VNiR as agreed
Equivalent material: JIS VCNiT1A, JIS VNiP, MIL 205
JIS H4501 Grade VNiR as agreed general
| Property |
Temperature |
Value |
Comment |
| Density |
23.0 °C |
Density of 8.8 g/cm³ |
Typical for Nickel Steel |
JIS H4501 Grade VNiR as agreed thermal
| Property |
Temperature |
Value |
Comment |
| Melting point |
- |
Melting point of 1316 - 1595 °C |
Typical for Nickel Steel |
| Specific heat capacity |
23.0 °C |
Specific heat capacity of 456 J/(kg·K) |
Typical for Nickel Steel |
| Thermal conductivity |
23.0 °C |
Thermal conductivity of 10 - 50 W/(m·K) |
Typical for Nickel Steel |
JIS H4501 Grade VNiR as agreed mechanical
| Property |
Temperature |
Value |
Comment |
| Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Nickel Steel |
| Elongation |
23.0 °C |
Elongation of 35 % |
- |
| Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Nickel Steel |
| Shear modulus |
23.0 °C |
Shear modulus of 76 GPa |
Typical for Nickel Steel |
| Tensile strength |
23.0 °C |
Tensile strength of 490 MPa |
- |