JIS G5111 Grade SCNCrM2A
JIS G5111 Grade SCNCrM2A general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
JIS G5111 Grade SCNCrM2A thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Melting point | - | Melting point of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |
JIS G5111 Grade SCNCrM2A mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Elongation A5 | 23.0 °C | Elongation A5 of 9 % | - |
Hardness, Brinell | 23.0 °C | Hardness, Brinell of 223 [-] | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Reduction of area | 23.0 °C | Reduction of area of 20 % | - |
Tensile strength | 23.0 °C | Tensile strength of 780 MPa | - |
Yield strength Rp0.2 | 23.0 °C | Yield strength Rp0.2 of 590 MPa | - |