JIS G5111 Grade SCMnCr4B
JIS G5111 Grade SCMnCr4B general
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for Chromium Steel |
JIS G5111 Grade SCMnCr4B thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 9.4E-6 - 1.5E-5 1/K | Typical for Chromium Steel |
| Melting point | - | Melting point of 1382 - 1529 °C | Typical for Chromium Steel |
| Specific heat capacity | 23.0 °C | Specific heat capacity of 440 - 494 J/(kg·K) | Typical for Chromium Steel |
| Thermal conductivity | 23.0 °C | Thermal conductivity of 23 - 50 W/(m·K) | Typical for Chromium Steel |
JIS G5111 Grade SCMnCr4B mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Chromium Steel |
| Elongation A5 | 23.0 °C | Elongation A5 of 13 % | - |
| Hardness, Brinell | 23.0 °C | Hardness, Brinell of 223 [-] | - |
| Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Chromium Steel |
| Reduction of area | 23.0 °C | Reduction of area of 25 % | - |
| Tensile strength | 23.0 °C | Tensile strength of 740 MPa | - |
| Yield strength Rp0.2 | 23.0 °C | Yield strength Rp0.2 of 540 MPa | - |