JIS G4902 Grade NCF750 solution treated
JIS G4902 Grade NCF750 solution treated general
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Density | 23.0 °C | Density of 8.8 g/cm³ | Typical for Nickel Steel |
JIS G4902 Grade NCF750 solution treated thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Melting point | - | Melting point of 1316 - 1595 °C | Typical for Nickel Steel |
| Specific heat capacity | 23.0 °C | Specific heat capacity of 456 J/(kg·K) | Typical for Nickel Steel |
| Thermal conductivity | 23.0 °C | Thermal conductivity of 10 - 50 W/(m·K) | Typical for Nickel Steel |
JIS G4902 Grade NCF750 solution treated mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Nickel Steel |
| Elongation A5 | 23.0 °C | Elongation A5 of 18 - 40 % | - |
| Hardness, Brinell | 23.0 °C | Hardness, Brinell of 302 - 363 [-] | - |
| Hardness, Rockwell C | 23.0 °C | Hardness, Rockwell C of 32 - 40 [-] | - |
| Hardness, Vickers | 23.0 °C | Hardness, Vickers of 313 - 382 [-] | - |
| Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Nickel Steel |
| Shear modulus | 23.0 °C | Shear modulus of 76 GPa | Typical for Nickel Steel |
| Tensile strength | 23.0 °C | Tensile strength of 890 - 1170 MPa | - |
| Yield strength Rp0.2 | 23.0 °C | Yield strength Rp0.2 of 795 MPa | - |