JIS G4901 Grade NCF751 ageing treatment after solution treatment
JIS G4901 Grade NCF751 ageing treatment after solution treatment general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 8.8 g/cm³ | Typical for Nickel Steel |
JIS G4901 Grade NCF751 ageing treatment after solution treatment thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | - | Melting point of 1316 - 1595 °C | Typical for Nickel Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 456 J/(kg·K) | Typical for Nickel Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 10 - 50 W/(m·K) | Typical for Nickel Steel |
JIS G4901 Grade NCF751 ageing treatment after solution treatment mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Nickel Steel |
Elongation A5 | 23.0 °C | Elongation A5 of 8 % | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Nickel Steel |
Shear modulus | 23.0 °C | Shear modulus of 76 GPa | Typical for Nickel Steel |
Tensile strength | 23.0 °C | Tensile strength of 960 MPa | - |
Yield strength Rp0.2 | 23.0 °C | Yield strength Rp0.2 of 615 MPa | - |