JIS G4805 Grade 17MnCr5 annealed (soft annealed)

Equivalent material: DIN 1.3521, DIN 17MnCr5, EN 1.3521, ISO 17MnCr5

JIS G4805 Grade 17MnCr5 annealed (soft annealed) general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Chromium Steel

JIS G4805 Grade 17MnCr5 annealed (soft annealed) thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 9.4E-6 - 1.5E-5 1/K Typical for Chromium Steel
Melting point - Melting point of 1382 - 1529 °C Typical for Chromium Steel
Specific heat capacity 23.0 °C Specific heat capacity of 440 - 494 J/(kg·K) Typical for Chromium Steel
Thermal conductivity 23.0 °C Thermal conductivity of 23 - 50 W/(m·K) Typical for Chromium Steel

JIS G4805 Grade 17MnCr5 annealed (soft annealed) mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Chromium Steel
Hardness, Brinell 23.0 °C Hardness, Brinell of 207 [-] -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Chromium Steel