Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.9 - 8.2 g/cm³ |
Typical for Austenitic Stainless Steel |
JIS G4308 Grade SUS420F2 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K |
Typical for Austenitic Stainless Steel |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 J/(kg·K) |
Typical for Austenitic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
JIS G4308 Grade SUS420F2 chemical
Property |
Value |
Carbon |
Carbon of 0.26 - 0.43 % |
Chromium |
Chromium of 12 - 14 % |
Iron |
Iron of 82.6 - 87.69 % |
Lead |
Lead of 0.05 - 0.3 % |
Manganese |
Manganese of 1 % |
Nickel |
Nickel of 0.6 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 1 % |
Sulfur |
Sulfur of 0.03 % |
JIS G4308 Grade SUS420F2 electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
JIS G4308 Grade SUS420F2 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 195 GPa |
Typical for Austenitic Stainless Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Partner with us to pioneer new engineering solutions using our advanced steel technologies.
-- Our promise
Similar or equivalent steel materials
Get a quote