JIS G4103 Grade SNCM815
Equivalent material: DIN 1.6657, DIN 14NiCrMo13-4, AFNOR 14NiCrMo13-4, BS 832M13, BS 14NiCrMo13-4, UNI 14NiCrMo13-4, UNE 14NiCrMo131, AISI E9310H, SAE E9310H, EN 14NiCrMo13-4, EN 1.6657, UNS H93106
JIS G4103 Grade SNCM815 general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Nickel Chromium Molybdenum Steel |
JIS G4103 Grade SNCM815 thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K |
Typical for Nickel Chromium Molybdenum Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Nickel Chromium Molybdenum Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 448 - 670 J/(kg·K) |
Typical for Nickel Chromium Molybdenum Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 34 - 54 W/(m·K) |
Typical for Nickel Chromium Molybdenum Steel |
JIS G4103 Grade SNCM815 chemical
Property |
Value |
Carbon |
Carbon of 0.12 - 0.18 % |
Chromium |
Chromium of 0.7 - 1 % |
Iron |
Iron of 93.01 - 94.58 % |
Manganese |
Manganese of 0.3 - 0.6 % |
Molybdenum |
Molybdenum of 0.15 - 0.3 % |
Nickel |
Nickel of 4 - 4.5 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 0.15 - 0.35 % |
Sulfur |
Sulfur of 0.03 % |
JIS G4103 Grade SNCM815 mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Nickel Chromium Molybdenum Steel |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Nickel Chromium Molybdenum Steel |
Choose our top-tier steel products to elevate the quality and strength of your structures and equipment.
-- Our promise
Similar or equivalent steel materials
Get a quote