JIS G3566 Grade SWOSC-V cold-drawn and oil tempered

Equivalent material: AS 9254H, DIN 54SiCr6, BS 251A60, BS 251H60, EN 55SiCr6, ASTM 9254, AS 9254, EN 56SiCr7, AMS 9254, ASTM G92540

JIS G3566 Grade SWOSC-V cold-drawn and oil tempered general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for High Carbon Steel

JIS G3566 Grade SWOSC-V cold-drawn and oil tempered thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.32E-5 1/K Typical for High Carbon Steel
Max service temperature - Max service temperature of 500 °C Typical for Carbon Steel
Melting point - Melting point of 1289 - 1478 °C Typical for High Carbon Steel
Specific heat capacity 23.0 °C Specific heat capacity of 486 J/(kg·K) Typical for High Carbon Steel
Thermal conductivity 23.0 °C Thermal conductivity of 36 W/(m·K) Typical for High Carbon Steel

JIS G3566 Grade SWOSC-V cold-drawn and oil tempered electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m Typical for Carbon Steel

JIS G3566 Grade SWOSC-V cold-drawn and oil tempered mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for High Carbon Steel
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for High Carbon Steel
Shear modulus 23.0 °C Shear modulus of 81 GPa Typical for High Carbon Steel
Tensile strength 23.0 °C Tensile strength of 1961 MPa -