JIS G3507 Grade SWRCH20A
JIS G3507 Grade SWRCH20A general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for High Carbon Steel |
JIS G3507 Grade SWRCH20A thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1.32E-5 1/K | Typical for High Carbon Steel |
Max service temperature | - | Max service temperature of 500 °C | Typical for Carbon Steel |
Melting point | - | Melting point of 1289 - 1478 °C | Typical for High Carbon Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 486 J/(kg·K) | Typical for High Carbon Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 36 W/(m·K) | Typical for High Carbon Steel |
JIS G3507 Grade SWRCH20A chemical
Property | Value |
---|---|
Aluminium | Aluminium of 0.02 % |
Carbon | Carbon of 0.18 - 0.23 % |
Iron | Iron of 99 - 99.5 % |
Manganese | Manganese of 0.3 - 0.6 % |
Phosphorus | Phosphorus of 0.03 % |
Silicon | Silicon of 0.1 % |
Sulfur | Sulfur of 0.035 % |
JIS G3507 Grade SWRCH20A electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Electrical resistivity | 23.0 °C | Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
JIS G3507 Grade SWRCH20A mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for High Carbon Steel |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for High Carbon Steel |
Shear modulus | 23.0 °C | Shear modulus of 81 GPa | Typical for High Carbon Steel |
Rely on our strong, dependable steel to support your most critical applications.
-- Our promise