JIS G3317 Grade SZACD1 cold-rolled
Equivalent material: DIN 1.0918, EN 1.0918
JIS G3317 Grade SZACD1 cold-rolled general
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
JIS G3317 Grade SZACD1 cold-rolled thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1.33E-5 1/K | Typical for Manganese Steel |
| Melting point | - | Melting point of 1382 - 1529 °C | Typical for Manganese Steel |
| Specific heat capacity | 23.0 °C | Specific heat capacity of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
| Thermal conductivity | 23.0 °C | Thermal conductivity of 14 - 16 W/(m·K) | Typical for Manganese Steel |
JIS G3317 Grade SZACD1 cold-rolled mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Manganese Steel |
| Elongation A5 | 23.0 °C | Elongation A5 of 34 - 38 % | - |
| Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Manganese Steel |
| Tensile strength | 23.0 °C | Tensile strength of 270 MPa | - |