JIS G3222 Grade SFNCM980S
JIS G3222 Grade SFNCM980S general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
JIS G3222 Grade SFNCM980S thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Melting point | - | Melting point of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |
JIS G3222 Grade SFNCM980S mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Elongation A5 | 23.0 °C | Elongation A5 of 11 - 13 % | - |
Elongation A5, transverse | 23.0 °C | Elongation A5, transverse of 8 - 70 % | - |
Hardness, Brinell | 23.0 °C | Hardness, Brinell of 285 [-] | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Reduction of area | 23.0 °C | Reduction of area of 34 - 39 % | - |
Reduction of area, transverse | 23.0 °C | Reduction of area, transverse of 23 - 24 % | - |
Tensile strength | 23.0 °C | Tensile strength of 980 - 1130 MPa | - |
Yield strength | 23.0 °C | Yield strength of 755 - 785 MPa | - |