JIS G3221 Grade SFCM830D
JIS G3221 Grade SFCM830D general
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | Density of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
JIS G3221 Grade SFCM830D thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | Coefficient of thermal expansion of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Melting point | - | Melting point of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Specific heat capacity | 23.0 °C | Specific heat capacity of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Thermal conductivity | 23.0 °C | Thermal conductivity of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
JIS G3221 Grade SFCM830D mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | Elastic modulus of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Elongation A5, transverse | 23.0 °C | Elongation A5, transverse of 9 - 13 % | - |
Hardness, Brinell | 23.0 °C | Hardness, Brinell of 241 [-] | - |
Poisson's ratio | 23.0 °C | Poisson's ratio of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Reduction of area | 23.0 °C | Reduction of area of 30 - 35 % | - |
Reduction of area, transverse | 23.0 °C | Reduction of area, transverse of 30 - 35 % | - |
Tensile strength | 23.0 °C | Tensile strength of 830 - 980 MPa | - |
Yield strength | 23.0 °C | Yield strength of 580 - 625 MPa | - |
Trust our expertise to deliver precision-engineered steel solutions that meet the highest industry standards.
-- Our promise
Get a quote