JIS G3214 Grade SUSF316L
Equivalent material: GB/T 00Cr17Ni14Mo2, GB/T 00Cr17Ni14Mo2-Q, GB/T 00Cr17Ni14Mo2-R, GB 00Cr17Ni14Mo2, GB 00Cr17Ni14Mo3, GOST 03Х17Н14М3, GOST 03H17N14M3, AS 316L, DIN X2CrNiMo17132, DIN X2CrNiMo18143, EN X2CrNiMo17-12-2, NF Z2CN18-10M, NF Z2CND17-12, NF Z2CND17-13, NF Z3CN19-9M, NF Z3CND20-10M, NF Z2CND18-12M, NF Z3CND19-10M, NF Z3CND17-11-02, NF Z3CND17-12-03, NF Z3CND18-12-03, NF Z3CND18-12-02, NF Z3CND18-14-03, NF Z3CND17-12-02FF, NF Z2CND18-13, BS 316S12, BS 316S11, BS 316S31, BS S.537, BS T.75, BS 316S13, BS 304C12, BS 316C12, BS 316S42, BS 316S24, BS 316S29, BS LW22, BS LWCF22, IS 02Cr17Ni12Mo2, IS O2Cr17Ni12Mo2, UNI GX2CrNiMo1911, UNI X2CrNiMo1712, UNI X2CrNiMo1713, UNI X2CrNiMo1713KG, UNI X2CrNiMo1713KW, ÖNORM X2CrNiMo17132KKW, ÖNORM X2CrNiMo18143KW, UNE AM-X2CrNiMo1911, UNE AM-X2CrNi1910, UNE X2CrNiMo17123, UNE X2CrNiMo17132, UNE X2CrNiMo17133, UNE F.310.K, SIS 2348-02, SIS 2348-22, SIS 2348-23, SIS 2348-24, SIS 2348-25, SIS 2348-26, SIS 2348-27, SIS 2348-28, SIS 2348-29, SIS 2348, SIS 2353, AMS 5507, AMS 5653, ASME 316L, ASTM TP316L, ASTM 316L, ASTM CR316L, ASTM WP316L, ASTM 18Cr 8Ni Mod. with Mo low C, ASTM F316L, ASTM MT316L, ASTM CF3MN, MIL 316L, JIS SUS316LTBS, JIS SUS316LTP, JIS SUS316TiTP, JIS SUS316L, JIS SCS16, AISI 316L, SAE 316L, EN X2CrNiMo18-14-3, DIN 1.4432, AFNOR Z3CND17-12-03, JIS SUS316LFB, EN X2CrNiMo17-12-3, EN 1.4432, GOST 06Ch17N13M3-WD, UNS S31603
JIS G3214 Grade SUSF316L general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.9 - 8.2 g/cm³ |
Typical for Austenitic Stainless Steel |
JIS G3214 Grade SUSF316L thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K |
Typical for Austenitic Stainless Steel |
Melting point |
- |
Melting point of 1230 - 1480 °C |
Typical for Austenitic Stainless Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 440 J/(kg·K) |
Typical for Austenitic Stainless Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 11 - 21 W/(m·K) |
Typical for Austenitic Stainless Steel |
JIS G3214 Grade SUSF316L electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 8.5E-7 Ω·m |
Typical for Austenitic Stainless Steel |
JIS G3214 Grade SUSF316L mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 195 GPa |
Typical for Austenitic Stainless Steel |
Elongation A5 |
23.0 °C |
Elongation A5 of 29 % |
- |
Hardness, Brinell |
23.0 °C |
Hardness, Brinell of 187 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Austenitic Stainless Steel |
Reduction of area |
23.0 °C |
Reduction of area of 45 - 50 % |
- |
Shear modulus |
23.0 °C |
Shear modulus of 77 GPa |
Typical for Austenitic Stainless Steel |
Tensile strength |
23.0 °C |
Tensile strength of 450 - 480 MPa |
- |
Yield strength Rp0.2 |
23.0 °C |
Yield strength Rp0.2 of 175 MPa |
- |