ISO 4957 Grade X45NiCrMo4 quenched and tempered (+QT)

ISO 4957 Grade X45NiCrMo4 quenched and tempered (+QT) introduction

Properties:
- tool steel for hardening in oil and on air
- well polishable
- excelent toughness
- fail-safe against high pressures and bending
Application:
- synthetic resin dies, tools for embossing, dies of any kind
- high loaded knifes for shears for cutting scrap

Equivalent material: ISO 40NiCrMoV4, UNI 40NiCrMoV16KU, DIN 45NiCrMo16, DIN 1.2767, AFNOR 45NiCrMo16, BS 45NiCrMo16, AISI 6F3, SAE 6F3, JIS SKT6, EN 45NiCrMo16, EN 40NiCrMoV16, EN 1.2767, ISO 45NiCrMo16

ISO 4957 Grade X45NiCrMo4 quenched and tempered (+QT) general

Property Temperature Value
Density 20.0 °C Density of 7.86 g/cm³

ISO 4957 Grade X45NiCrMo4 quenched and tempered (+QT) thermal

Property Temperature Value Comment
Coefficient of thermal expansion 100.0 °C Coefficient of thermal expansion of 1.15E-5 1/K -
- 200.0 °C Coefficient of thermal expansion of 1.2E-5 1/K -
- 300.0 °C Coefficient of thermal expansion of 1.24E-5 1/K -
- 400.0 °C Coefficient of thermal expansion of 1.28E-5 1/K -
- 500.0 °C Coefficient of thermal expansion of 1.31E-5 1/K -
- 600.0 °C Coefficient of thermal expansion of 1.35E-5 1/K -
Melting point - Melting point of 1370 - 1425 °C Typical for Tool And Machining Steel
Specific heat capacity 20.0 °C Specific heat capacity of 464 J/(kg·K) -
- 100.0 °C Specific heat capacity of 479 J/(kg·K) -
- 200.0 °C Specific heat capacity of 496 J/(kg·K) -
- 300.0 °C Specific heat capacity of 513 J/(kg·K) -
- 400.0 °C Specific heat capacity of 532 J/(kg·K) -
Thermal conductivity 20.0 °C Thermal conductivity of 32.9 W/(m·K) -
- 100.0 °C Thermal conductivity of 34.2 W/(m·K) -
- 200.0 °C Thermal conductivity of 34.8 W/(m·K) -
- 300.0 °C Thermal conductivity of 34.4 W/(m·K) -
- 400.0 °C Thermal conductivity of 33.3 W/(m·K) -
Thermal diffusivity 20.0 °C Thermal diffusivity of 9 mm²/s -
- 100.0 °C Thermal diffusivity of 8.8 mm²/s -
- 200.0 °C Thermal diffusivity of 8.5 mm²/s -
- 300.0 °C Thermal diffusivity of 7.8 mm²/s -
- 400.0 °C Thermal diffusivity of 7.1 mm²/s -

ISO 4957 Grade X45NiCrMo4 quenched and tempered (+QT) chemical

Property Value
Carbon Carbon of 0.4 - 0.5 %
Chromium Chromium of 1.2 - 1.5 %
Manganese Manganese of 0.15 - 0.45 %
Molybdenum Molybdenum of 0.15 - 0.35 %
Nickel Nickel of 3.8 - 4.3 %
Phosphorus Phosphorus of 0.03 %
Silicon Silicon of 0.1 - 0.4 %
Sulfur Sulfur of 0.03 %
Tungsten Tungsten of 0.4 - 0.6 %

ISO 4957 Grade X45NiCrMo4 quenched and tempered (+QT) electrical

Property Temperature Value
Electrical resistivity 20.0 °C Electrical resistivity of 3.17E-7 Ω·m
- 100.0 °C Electrical resistivity of 3.74E-7 Ω·m
- 200.0 °C Electrical resistivity of 4.54E-7 Ω·m
- 300.0 °C Electrical resistivity of 5.46E-7 Ω·m
- 400.0 °C Electrical resistivity of 6.53E-7 Ω·m

ISO 4957 Grade X45NiCrMo4 quenched and tempered (+QT) mechanical

Property Temperature Value Comment
Elastic modulus 20.0 °C Elastic modulus of 207 GPa -
- 100.0 °C Elastic modulus of 203 GPa -
- 200.0 °C Elastic modulus of 197 GPa -
- 300.0 °C Elastic modulus of 189 GPa -
- 400.0 °C Elastic modulus of 181 GPa -
- 500.0 °C Elastic modulus of 172 GPa -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Tool And Machining Steel
Shear modulus 23.0 °C Shear modulus of 79 GPa Typical for Tool And Machining Steel

We set new standards in steel manufacturing, pushing boundaries to deliver exceptional quality.

-- Our promise

Get a quote