ISO 4957 Grade S6-5-3 quenched (+Q)

ISO 4957 Grade S6-5-3 quenched (+Q) introduction

Very wear resistant W-Mo-V high speed steel with highest cut accuracy and good toughness.
Application: machining of hard materials at high cutting speed, fine-cutting precision tools, high performance spiral drills, reamer, cutter

Equivalent material: GB W6Mo5Cr4V3, ISO HS6-5-3, JIS SKH52, SS 2725, UNE F.5606, MSZ R13, SAE M3, DIN HS6-5-3, DIN X125WMo6.5, DIN 1.3344, AFNOR Z120WDCV06-05-04-03, AFNOR HS6-5-3, AFNOR 6-5-3, BS HS6-5-3, AISI M3, AISI M3Class1, AISI M3Class2, SAE M3Class1, SAE M3Class2, JIS SKH53, EN HS6-5-3, EN 1.3344, GOST R6M5F3, GB/T T66543, GB/T W6Mo5Cr4V3, ASTM Type M3, UNS T11313, UNS T11323

ISO 4957 Grade S6-5-3 quenched (+Q) general

Property Temperature Value
Density 20.0 °C Density of 8.12 g/cm³

ISO 4957 Grade S6-5-3 quenched (+Q) thermal

Property Temperature Value Comment
Coefficient of thermal expansion -100.0 °C Coefficient of thermal expansion of 9.6E-6 1/K -
- 20.0 °C Coefficient of thermal expansion of 1.05E-5 1/K -
- 100.0 °C Coefficient of thermal expansion of 1.11E-5 1/K -
- 200.0 °C Coefficient of thermal expansion of 1.16E-5 1/K -
- 300.0 °C Coefficient of thermal expansion of 1.2E-5 1/K -
- 400.0 °C Coefficient of thermal expansion of 1.24E-5 1/K -
- 500.0 °C Coefficient of thermal expansion of 1.27E-5 1/K -
- 600.0 °C Coefficient of thermal expansion of 1.3E-5 1/K -
Melting point - Melting point of 1370 - 1425 °C Typical for Tool And Machining Steel
Specific heat capacity 23.0 °C Specific heat capacity of 420 - 460 J/(kg·K) Typical for Tool And Machining Steel
Thermal conductivity 20.0 °C Thermal conductivity of 27.6 W/(m·K) -
- 100.0 °C Thermal conductivity of 27.9 W/(m·K) -
- 200.0 °C Thermal conductivity of 27.7 W/(m·K) -
- 300.0 °C Thermal conductivity of 27.5 W/(m·K) -
- 400.0 °C Thermal conductivity of 27 W/(m·K) -
- 500.0 °C Thermal conductivity of 26.6 W/(m·K) -
- 600.0 °C Thermal conductivity of 26.1 W/(m·K) -

ISO 4957 Grade S6-5-3 quenched (+Q) chemical

Property Value
Carbon Carbon of 1.17 - 1.27 %
Chromium Chromium of 3.8 - 4.5 %
Manganese Manganese of 0.4 %
Molybdenum Molybdenum of 4.7 - 5.2 %
Phosphorus Phosphorus of 0.03 %
Silicon Silicon of 0.45 %
Sulfur Sulfur of 0.03 %
Tungsten Tungsten of 6 - 6.7 %
Vanadium Vanadium of 2.7 - 3.2 %

ISO 4957 Grade S6-5-3 quenched (+Q) electrical

Property Temperature Value
Electrical resistivity 20.0 °C Electrical resistivity of 5.24E-7 Ω·m
- 100.0 °C Electrical resistivity of 5.81E-7 Ω·m
- 200.0 °C Electrical resistivity of 6.64E-7 Ω·m
- 300.0 °C Electrical resistivity of 7.51E-7 Ω·m
- 400.0 °C Electrical resistivity of 8.44E-7 Ω·m
- 500.0 °C Electrical resistivity of 9.41E-7 Ω·m
- 600.0 °C Electrical resistivity of 1.04E-6 Ω·m

ISO 4957 Grade S6-5-3 quenched (+Q) mechanical

Property Temperature Value Comment
Elastic modulus 20.0 °C Elastic modulus of 224 GPa -
- 100.0 °C Elastic modulus of 220 GPa -
- 200.0 °C Elastic modulus of 214 GPa -
- 300.0 °C Elastic modulus of 207 GPa -
- 400.0 °C Elastic modulus of 199 GPa -
- 500.0 °C Elastic modulus of 191 GPa -
- 600.0 °C Elastic modulus of 180 GPa -
Poisson's ratio 20.0 °C Poisson's ratio of 0.28 [-] -
Shear modulus 23.0 °C Shear modulus of 79 GPa Typical for Tool And Machining Steel