ISO 4957 Grade S3-3-2
ISO 4957 Grade S3-3-2 introduction
Application: spiral drills, reamer
Equivalent material: CSN 19820, GOST 11R3AM3F2, UNI HS3-3-2, STAS Rp9, DIN HS3-3-2, DIN 1.3333, AFNOR HS3-3-2, BS HS3-3-2, EN HS3-3-2, EN 1.3333, ISO HS3-3-2, GB/T T63342, GB/T W3Mo3Cr4V2
ISO 4957 Grade S3-3-2 general
| Property | Temperature | Value |
|---|---|---|
| Density | 20.0 °C | Density of 8.12 g/cm³ |
ISO 4957 Grade S3-3-2 thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Coefficient of thermal expansion | -100.0 °C | Coefficient of thermal expansion of 9.6E-6 1/K | - |
| - | 20.0 °C | Coefficient of thermal expansion of 1.05E-5 1/K | - |
| - | 100.0 °C | Coefficient of thermal expansion of 1.11E-5 1/K | - |
| - | 200.0 °C | Coefficient of thermal expansion of 1.16E-5 1/K | - |
| - | 300.0 °C | Coefficient of thermal expansion of 1.2E-5 1/K | - |
| - | 400.0 °C | Coefficient of thermal expansion of 1.24E-5 1/K | - |
| - | 500.0 °C | Coefficient of thermal expansion of 1.27E-5 1/K | - |
| - | 600.0 °C | Coefficient of thermal expansion of 1.3E-5 1/K | - |
| Melting point | - | Melting point of 1370 - 1425 °C | Typical for Tool And Machining Steel |
| Specific heat capacity | 23.0 °C | Specific heat capacity of 420 - 460 J/(kg·K) | Typical for Tool And Machining Steel |
| Thermal conductivity | 20.0 °C | Thermal conductivity of 27.6 W/(m·K) | - |
| - | 100.0 °C | Thermal conductivity of 27.9 W/(m·K) | - |
| - | 200.0 °C | Thermal conductivity of 27.7 W/(m·K) | - |
| - | 300.0 °C | Thermal conductivity of 27.5 W/(m·K) | - |
| - | 400.0 °C | Thermal conductivity of 27 W/(m·K) | - |
| - | 500.0 °C | Thermal conductivity of 26.6 W/(m·K) | - |
| - | 600.0 °C | Thermal conductivity of 26.1 W/(m·K) | - |
ISO 4957 Grade S3-3-2 chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.95 - 1.03 % |
| Chromium | Chromium of 3.8 - 4.5 % |
| Manganese | Manganese of 0.4 % |
| Molybdenum | Molybdenum of 2.5 - 2.9 % |
| Phosphorus | Phosphorus of 0.03 % |
| Silicon | Silicon of 0.4 % |
| Sulfur | Sulfur of 0.45 % |
| Tungsten | Tungsten of 2.7 - 3 % |
| Vanadium | Vanadium of 2.2 - 2.5 % |
ISO 4957 Grade S3-3-2 electrical
| Property | Temperature | Value |
|---|---|---|
| Electrical resistivity | 20.0 °C | Electrical resistivity of 5.24E-7 Ω·m |
| - | 100.0 °C | Electrical resistivity of 5.81E-7 Ω·m |
| - | 200.0 °C | Electrical resistivity of 6.64E-7 Ω·m |
| - | 300.0 °C | Electrical resistivity of 7.51E-7 Ω·m |
| - | 400.0 °C | Electrical resistivity of 8.44E-7 Ω·m |
| - | 500.0 °C | Electrical resistivity of 9.41E-7 Ω·m |
| - | 600.0 °C | Electrical resistivity of 1.04E-6 Ω·m |
ISO 4957 Grade S3-3-2 mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Elastic modulus | 20.0 °C | Elastic modulus of 224 GPa | - |
| - | 100.0 °C | Elastic modulus of 220 GPa | - |
| - | 200.0 °C | Elastic modulus of 214 GPa | - |
| - | 300.0 °C | Elastic modulus of 207 GPa | - |
| - | 400.0 °C | Elastic modulus of 199 GPa | - |
| - | 500.0 °C | Elastic modulus of 191 GPa | - |
| - | 600.0 °C | Elastic modulus of 180 GPa | - |
| Poisson's ratio | 20.0 °C | Poisson's ratio of 0.28 [-] | - |
| Shear modulus | 23.0 °C | Shear modulus of 79 GPa | Typical for Tool And Machining Steel |
Our steel embodies these qualities to deliver exceptional results.
-- Our promise