ISO 4957 Grade S2-10-1-8 soft annealed (+A)
ISO 4957 Grade S2-10-1-8 soft annealed (+A) introduction
High wear resistance, hot hardness and toughness.
Application: die and grave cutter, tool bits for machining, as cold work steel for dies
Equivalent material: AFNOR Z110DKCWV09-08-04-02-01, BS BM42, GOST R2AM9K5, ISO HS2-9-1-8, UNI HS2-9-1-8, JIS SKH59, PN SK8M, SS 2716, UNE F.5617, MSZ R11, AISI M42, DIN HS2-9-1-8, DIN 1.3247, AFNOR HS2-9-1-8, AFNOR 2-9-1-8, BS HS2-9-1-8, SS 2-10-1-8, UNE M41, SAE M42, EN HS2-9-1-8, EN 1.3247, GB/T T72948, GB/T W2Mo9Cr4VCo8, ASTM Type M42, UNS T11342
ISO 4957 Grade S2-10-1-8 soft annealed (+A) general
Property |
Temperature |
Value |
Density |
20.0 °C |
Density of 8.12 g/cm³ |
ISO 4957 Grade S2-10-1-8 soft annealed (+A) thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
-100.0 °C |
Coefficient of thermal expansion of 9.6E-6 1/K |
- |
- |
20.0 °C |
Coefficient of thermal expansion of 1.05E-5 1/K |
- |
- |
100.0 °C |
Coefficient of thermal expansion of 1.11E-5 1/K |
- |
- |
200.0 °C |
Coefficient of thermal expansion of 1.16E-5 1/K |
- |
- |
300.0 °C |
Coefficient of thermal expansion of 1.2E-5 1/K |
- |
- |
400.0 °C |
Coefficient of thermal expansion of 1.24E-5 1/K |
- |
- |
500.0 °C |
Coefficient of thermal expansion of 1.27E-5 1/K |
- |
- |
600.0 °C |
Coefficient of thermal expansion of 1.3E-5 1/K |
- |
Melting point |
- |
Melting point of 1370 - 1425 °C |
Typical for Tool And Machining Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 420 - 460 J/(kg·K) |
Typical for Tool And Machining Steel |
Thermal conductivity |
20.0 °C |
Thermal conductivity of 27.6 W/(m·K) |
- |
- |
100.0 °C |
Thermal conductivity of 27.9 W/(m·K) |
- |
- |
200.0 °C |
Thermal conductivity of 27.7 W/(m·K) |
- |
- |
300.0 °C |
Thermal conductivity of 27.5 W/(m·K) |
- |
- |
400.0 °C |
Thermal conductivity of 27 W/(m·K) |
- |
- |
500.0 °C |
Thermal conductivity of 26.6 W/(m·K) |
- |
- |
600.0 °C |
Thermal conductivity of 26.1 W/(m·K) |
- |
ISO 4957 Grade S2-10-1-8 soft annealed (+A) chemical
Property |
Value |
Carbon |
Carbon of 1.05 - 1.12 % |
Chromium |
Chromium of 3.6 - 4.4 % |
Cobalt |
Cobalt of 7.5 - 8.5 % |
Manganese |
Manganese of 0.4 % |
Molybdenum |
Molybdenum of 9 - 10 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 0.45 % |
Sulfur |
Sulfur of 0.03 % |
Tungsten |
Tungsten of 1.2 - 1.8 % |
Vanadium |
Vanadium of 1 - 1.3 % |
ISO 4957 Grade S2-10-1-8 soft annealed (+A) electrical
Property |
Temperature |
Value |
Electrical resistivity |
20.0 °C |
Electrical resistivity of 5.24E-7 Ω·m |
- |
100.0 °C |
Electrical resistivity of 5.81E-7 Ω·m |
- |
200.0 °C |
Electrical resistivity of 6.64E-7 Ω·m |
- |
300.0 °C |
Electrical resistivity of 7.51E-7 Ω·m |
- |
400.0 °C |
Electrical resistivity of 8.44E-7 Ω·m |
- |
500.0 °C |
Electrical resistivity of 9.41E-7 Ω·m |
- |
600.0 °C |
Electrical resistivity of 1.04E-6 Ω·m |
ISO 4957 Grade S2-10-1-8 soft annealed (+A) mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
20.0 °C |
Elastic modulus of 224 GPa |
- |
- |
100.0 °C |
Elastic modulus of 220 GPa |
- |
- |
200.0 °C |
Elastic modulus of 214 GPa |
- |
- |
300.0 °C |
Elastic modulus of 207 GPa |
- |
- |
400.0 °C |
Elastic modulus of 199 GPa |
- |
- |
500.0 °C |
Elastic modulus of 191 GPa |
- |
- |
600.0 °C |
Elastic modulus of 180 GPa |
- |
Poisson's ratio |
20.0 °C |
Poisson's ratio of 0.28 [-] |
- |
Shear modulus |
23.0 °C |
Shear modulus of 79 GPa |
Typical for Tool And Machining Steel |