ISO 4957 Grade 45CrMoV7
ISO 4957 Grade 45CrMoV7 introduction
bils of any kind for hardening on air wihtout tempering
Equivalent material: DIN 1.2332, EN 1.2332
ISO 4957 Grade 45CrMoV7 general
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | Density of 7.83 g/cm³ |
ISO 4957 Grade 45CrMoV7 thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | -100.0 °C | Coefficient of thermal expansion of 1.05E-5 1/K | - |
- | 20.0 °C | Coefficient of thermal expansion of 1.15E-5 1/K | - |
- | 100.0 °C | Coefficient of thermal expansion of 1.21E-5 1/K | - |
- | 200.0 °C | Coefficient of thermal expansion of 1.27E-5 1/K | - |
- | 300.0 °C | Coefficient of thermal expansion of 1.32E-5 1/K | - |
- | 400.0 °C | Coefficient of thermal expansion of 1.36E-5 1/K | - |
- | 500.0 °C | Coefficient of thermal expansion of 1.4E-5 1/K | - |
- | 600.0 °C | Coefficient of thermal expansion of 1.44E-5 1/K | - |
Melting point | - | Melting point of 1370 - 1425 °C | Typical for Tool And Machining Steel |
Specific heat capacity | -100.0 °C | Specific heat capacity of 423 J/(kg·K) | - |
- | 20.0 °C | Specific heat capacity of 461 J/(kg·K) | - |
- | 100.0 °C | Specific heat capacity of 479 J/(kg·K) | - |
- | 200.0 °C | Specific heat capacity of 499 J/(kg·K) | - |
- | 300.0 °C | Specific heat capacity of 517 J/(kg·K) | - |
- | 400.0 °C | Specific heat capacity of 536 J/(kg·K) | - |
- | 500.0 °C | Specific heat capacity of 558 J/(kg·K) | - |
- | 600.0 °C | Specific heat capacity of 587 J/(kg·K) | - |
Thermal conductivity | 20.0 °C | Thermal conductivity of 45.1 W/(m·K) | - |
- | 100.0 °C | Thermal conductivity of 45.1 W/(m·K) | - |
- | 200.0 °C | Thermal conductivity of 44.1 W/(m·K) | - |
- | 300.0 °C | Thermal conductivity of 41.9 W/(m·K) | - |
- | 400.0 °C | Thermal conductivity of 39.4 W/(m·K) | - |
- | 500.0 °C | Thermal conductivity of 36.9 W/(m·K) | - |
- | 600.0 °C | Thermal conductivity of 34.4 W/(m·K) | - |
Thermal diffusivity | 20.0 °C | Thermal diffusivity of 12.5 mm²/s | - |
- | 100.0 °C | Thermal diffusivity of 11.6 mm²/s | - |
- | 200.0 °C | Thermal diffusivity of 10.6 mm²/s | - |
- | 300.0 °C | Thermal diffusivity of 9.5 mm²/s | - |
- | 400.0 °C | Thermal diffusivity of 8.4 mm²/s | - |
- | 500.0 °C | Thermal diffusivity of 7.1 mm²/s | - |
- | 600.0 °C | Thermal diffusivity of 5.8 mm²/s | - |
ISO 4957 Grade 45CrMoV7 chemical
Property | Value |
---|---|
Carbon | Carbon of 0.42 - 0.47 % |
Chromium | Chromium of 1.7 - 1.9 % |
Manganese | Manganese of 0.85 - 1 % |
Molybdenum | Molybdenum of 0.25 - 0.3 % |
Phosphorus | Phosphorus of 0.03 % |
Silicon | Silicon of 0.2 - 0.3 % |
Sulfur | Sulfur of 0.03 % |
Vanadium | Vanadium of 0.05 % |
ISO 4957 Grade 45CrMoV7 electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | Electrical resistivity of 2.31E-7 Ω·m |
- | 100.0 °C | Electrical resistivity of 2.84E-7 Ω·m |
- | 200.0 °C | Electrical resistivity of 3.58E-7 Ω·m |
- | 300.0 °C | Electrical resistivity of 4.48E-7 Ω·m |
- | 400.0 °C | Electrical resistivity of 5.52E-7 Ω·m |
- | 500.0 °C | Electrical resistivity of 6.71E-7 Ω·m |
- | 600.0 °C | Electrical resistivity of 8.06E-7 Ω·m |
ISO 4957 Grade 45CrMoV7 mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | -100.0 °C | Elastic modulus of 217 GPa | - |
- | 20.0 °C | Elastic modulus of 212 GPa | - |
- | 100.0 °C | Elastic modulus of 207 GPa | - |
- | 200.0 °C | Elastic modulus of 199 GPa | - |
- | 300.0 °C | Elastic modulus of 192 GPa | - |
- | 400.0 °C | Elastic modulus of 184 GPa | - |
- | 500.0 °C | Elastic modulus of 175 GPa | - |
- | 600.0 °C | Elastic modulus of 164 GPa | - |
Poisson's ratio | 20.0 °C | Poisson's ratio of 0.28 [-] | - |
Shear modulus | 23.0 °C | Shear modulus of 79 GPa | Typical for Tool And Machining Steel |