EN 10277-2 Grade E335GC as rolled and turned (+SH)
EN 10277-2 Grade E335GC as rolled and turned (+SH) introduction
E335GC is applicated as cold drawing grade. The steel is used for wear and strength loaded parts (bolts, shafts, spindles, axles, wedges). It is surface hardenable. As a bright steel product it is used in the form of bars, bright, straight, in various conditions (see DIN EN 10277 : 1999-10).
Equivalent material: DIN ZSt60-2, DIN 1.0543, DIN E335GC, AFNOR E335GC, BS E335GC, JIS SM570, EN 1.0543, ISO Fe 590, GB HRB 335, ASTM Grade 2
EN 10277-2 Grade E335GC as rolled and turned (+SH) general
Property |
Temperature |
Value |
Density |
20.0 °C |
Density of 7.85 g/cm³ |
EN 10277-2 Grade E335GC as rolled and turned (+SH) thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
100.0 °C |
Coefficient of thermal expansion of 1.11E-5 1/K |
- |
- |
200.0 °C |
Coefficient of thermal expansion of 1.21E-5 1/K |
- |
- |
300.0 °C |
Coefficient of thermal expansion of 1.29E-5 1/K |
- |
- |
400.0 °C |
Coefficient of thermal expansion of 1.35E-5 1/K |
- |
Max service temperature |
- |
Max service temperature of 500 °C |
Typical for Carbon Steel |
Melting point |
- |
Melting point of 1380 - 1514 °C |
Typical for Medium Carbon Steel |
Specific heat capacity |
20.0 °C |
Specific heat capacity of 450 J/(kg·K) |
- |
Thermal conductivity |
20.0 °C |
Thermal conductivity of 54 W/(m·K) |
- |
- |
100.0 °C |
Thermal conductivity of 50.7 W/(m·K) |
- |
- |
200.0 °C |
Thermal conductivity of 46.9 W/(m·K) |
- |
- |
300.0 °C |
Thermal conductivity of 41.5 W/(m·K) |
- |
- |
400.0 °C |
Thermal conductivity of 39.4 W/(m·K) |
- |
EN 10277-2 Grade E335GC as rolled and turned (+SH) magnetic
Property |
Value |
Nitrogen |
Nitrogen of 9E-3 % |
Phosphorus |
Phosphorus of 0.05 % |
Sulfur |
Sulfur of 0.045 % |
EN 10277-2 Grade E335GC as rolled and turned (+SH) electrical
Property |
Temperature |
Value |
Electrical resistivity |
20.0 °C |
Electrical resistivity of 2E-7 Ω·m |
EN 10277-2 Grade E335GC as rolled and turned (+SH) mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
20.0 °C |
Elastic modulus of 210 GPa |
- |
- |
100.0 °C |
Elastic modulus of 205 GPa |
- |
- |
200.0 °C |
Elastic modulus of 195 GPa |
- |
- |
300.0 °C |
Elastic modulus of 185 GPa |
- |
- |
400.0 °C |
Elastic modulus of 175 GPa |
- |
Hardness, Brinell |
20.0 °C |
Hardness, Brinell of 169 - 211 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Medium Carbon Steel |
Shear modulus |
20.0 °C |
Shear modulus of 81 GPa |
- |
Tensile strength |
20.0 °C |
Tensile strength of 570 - 710 MPa |
- |
Let our innovative steel solutions unleash your creativity and drive excellence in your industry.