EN 10270-2 Grade TDSiCr oil quenched and tempered
EN 10270-2 Grade TDSiCr oil quenched and tempered introduction
The round, oil hardened and tempered alloy steel wire TDSiCr with medium fatigue strength and high tensile strength is used mainly for torsion loaded springs (tension and compression springs).
It will be delivered in rings, in coils or as bars and, if not otherwise arranged, thin oiled.
Equivalent material: IS TDSiCr, ISO TDSiCr, DIN TD SiCr, AFNOR TDSiCr, BS TDSiCr
EN 10270-2 Grade TDSiCr oil quenched and tempered general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 g/cm³ |
Typical for Steel |
EN 10270-2 Grade TDSiCr oil quenched and tempered chemical
Property |
Value |
Carbon |
Carbon of 0.5 - 0.6 % |
Chromium |
Chromium of 0.5 - 0.8 % |
Copper |
Copper of 0.1 % |
Manganese |
Manganese of 0.5 - 0.9 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 1.2 - 1.6 % |
Sulfur |
Sulfur of 0.02 % |
EN 10270-2 Grade TDSiCr oil quenched and tempered mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
20.0 °C |
Elastic modulus of 206 GPa |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Steel |
Reduction of area |
20.0 °C |
Reduction of area of 35 - 50 % |
- |
Shear modulus |
20.0 °C |
Shear modulus of 79.5 - 81.5 GPa |
- |
Tensile strength |
20.0 °C |
Tensile strength of 1670 - 2230 MPa |
- |