EN 10270-2 Grade TDCrV oil quenched and tempered
EN 10270-2 Grade TDCrV oil quenched and tempered introduction
The round, oil hardened and tempered alloy steel wire TDCrV with medium fatigue strength and medium tensile strength is used mainly for torsion loaded springs (tension and compression springs).
It will be delivered in rings, in coils or as bars and, if not otherwise arranged, thin oiled.
Der runde, ölschlußvergütete Federdraht der Sorte TDCrV aus legiertem Stahl wird vorzugsweise verwendet für mittlere torsionsbeanspruchte Federn (Zug- und Druckfedern) oberhalb Raumtemperatur.
Der Draht wird in Ringen, auf Spulen oder in Stäben und, wenn nicht anders vereinbart, im leicht geölten Zustand geliefert.
Equivalent material: IS TDCrV-B, ISO TDCrV, DIN TD CrV, AFNOR TDCrV, BS TDCrV
EN 10270-2 Grade TDCrV oil quenched and tempered general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Chromium Vanadium Steel |
EN 10270-2 Grade TDCrV oil quenched and tempered thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.2E-5 1/K |
Typical for Chromium Vanadium Steel |
Melting point |
- |
Melting point of 1382 - 1529 °C |
Typical for Chromium Vanadium Steel |
EN 10270-2 Grade TDCrV oil quenched and tempered chemical
Property |
Value |
Carbon |
Carbon of 0.62 - 0.72 % |
Chromium |
Chromium of 0.4 - 0.6 % |
Copper |
Copper of 0.1 % |
Manganese |
Manganese of 0.5 - 0.9 % |
Phosphorus |
Phosphorus of 0.03 % |
Silicon |
Silicon of 0.15 - 0.3 % |
Sulfur |
Sulfur of 0.02 % |
Vanadium |
Vanadium of 0.15 - 0.25 % |
EN 10270-2 Grade TDCrV oil quenched and tempered mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
20.0 °C |
Elastic modulus of 206 GPa |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Chromium Vanadium Steel |
Reduction of area |
20.0 °C |
Reduction of area of 40 - 50 % |
- |
Shear modulus |
20.0 °C |
Shear modulus of 79.5 - 81.5 GPa |
- |
Tensile strength |
20.0 °C |
Tensile strength of 1390 - 2060 MPa |
- |