EN 10248-1 Grade S320GP hot rolled

Equivalent material: AFNOR E320SP, DIN 1.0046, DIN S320GP, AFNOR S320GP, BS S320GP, EN 1.0046

EN 10248-1 Grade S320GP hot rolled general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Low Carbon Steel

EN 10248-1 Grade S320GP hot rolled thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K Typical for Low Carbon Steel
Max service temperature - Max service temperature of 500 °C Typical for Carbon Steel
Melting point - Melting point of 1480 - 1526 °C Typical for Low Carbon Steel
Specific heat capacity 23.0 °C Specific heat capacity of 465 J/(kg·K) Typical for Low Carbon Steel
Thermal conductivity 23.0 °C Thermal conductivity of 25 - 93 W/(m·K) Typical for Low Carbon Steel

EN 10248-1 Grade S320GP hot rolled chemical

Property Value
Carbon Carbon of 0.24 %
Manganese Manganese of 1.6 %
Nitrogen Nitrogen of 9E-3 %
Phosphorus Phosphorus of 0.05 %
Silicon Silicon of 0.55 %
Sulfur Sulfur of 0.045 %

EN 10248-1 Grade S320GP hot rolled magnetic

Property Value Comment
Curie temperature Curie temperature of 770 °C Typical for Low Carbon Steel

EN 10248-1 Grade S320GP hot rolled electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m Typical for Carbon Steel

EN 10248-1 Grade S320GP hot rolled mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Low Carbon Steel
Elongation 20.0 °C Elongation of 23 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Low Carbon Steel
Shear modulus 23.0 °C Shear modulus of 82 GPa Typical for Low Carbon Steel
Tensile strength 20.0 °C Tensile strength of 440 MPa -
Yield strength 20.0 °C Yield strength of 320 MPa -

Trust is built on the reliability and strength of our steel products and services.

-- Our promise

Get a quote