The standard is applicable to steels for offshore structures, designed to operate in the offshore sector but not to steels supplied for the fabrication of subsea pipelines, risers, process equipment, process piping, and other utilities. It is primarily applicable to the North Sea Sector, but may also be applicable in other areas provided that due consideration is given to local conditions e.g. temperature.

Equivalent material: EN S460G1+M, DIN 1.8878, EN 1.8878

EN 10225 Grade S460G1 thermomechanically rolled general

Property Value Comment
Density Density of 7.8 g/cm³ Typical for Steel

EN 10225 Grade S460G1 thermomechanically rolled thermal

Property Value Comment
Coefficient of thermal expansion Coefficient of thermal expansion of 11.89 1/K Predicted Value
Specific heat capacity Specific heat capacity of 453.1 J/(kg·K) Predicted Value
Thermal conductivity Thermal conductivity of 37.03 W/(m·K) Predicted Value

EN 10225 Grade S460G1 thermomechanically rolled chemical

Property Value Condition Related Standards Shape
Aluminium Aluminium of 0.015 - 0.055 % thermomechanically rolled EN 10225 Sheet
Antimony Antimony of 0.01 % thermomechanically rolled EN 10225 Sheet
Arsenic Arsenic of 0.03 % thermomechanically rolled EN 10225 Sheet
Bismuth Bismuth of 0.01 % thermomechanically rolled EN 10225 Sheet
Boron Boron of 0.001 % thermomechanically rolled EN 10225 Sheet
Calcium Calcium of 0.005 % thermomechanically rolled EN 10225 Sheet
Carbon Carbon of 0.14 % thermomechanically rolled EN 10225 Sheet
Chromium Chromium of 0.25 % thermomechanically rolled EN 10225 Sheet
Copper Copper of 0.3 % thermomechanically rolled EN 10225 Sheet
Lead Lead of 0.01 % thermomechanically rolled EN 10225 Sheet
Manganese Manganese of 1.65 % thermomechanically rolled EN 10225 Sheet
Molybdenum Molybdenum of 0.25 % thermomechanically rolled EN 10225 Sheet
Nickel Nickel of 0.7 % thermomechanically rolled EN 10225 Sheet
Niobium Niobium of 0.04 % thermomechanically rolled EN 10225 Sheet
Nitrogen Nitrogen of 0.01 % thermomechanically rolled EN 10225 Sheet
Phosphorus Phosphorus of 0.02 % thermomechanically rolled EN 10225 Sheet
Silicon Silicon of 0.15 - 0.55 % thermomechanically rolled EN 10225 Sheet
Sulfur Sulfur of 0.01 % thermomechanically rolled EN 10225 Sheet
Tin Tin of 0.02 % thermomechanically rolled EN 10225 Sheet
Titanium Titanium of 0.025 % thermomechanically rolled EN 10225 Sheet
Vanadium Vanadium of 0.08 % thermomechanically rolled EN 10225 Sheet

EN 10225 Grade S460G1 thermomechanically rolled electrical

Property Value Comment
Electrical conductivity Electrical conductivity of 7 S/m Predicted Value
Electrical resistivity Electrical resistivity of 36 Ω·m Predicted Value

EN 10225 Grade S460G1 thermomechanically rolled mechanical

Property Temperature Value Condition Related Standards Shape Comment
Elastic modulus - Elastic modulus of 190 - 210 GPa - - - Typical for Steel
Elongation - Elongation of 15.1 % - - - Predicted Value, A200
- - Elongation of 15.2 % - - - Predicted Value, A80
- - Elongation of 18.1 % - - - Predicted Value, Transverse
- - Elongation of 20.5 % - - - Predicted Value, A5
- - Elongation of 20.7 % - - - Predicted Value, A80 Transverse
- - Elongation of 23.9 % - - - Predicted Value, A50
- 20 °C Elongation of 17 % thermomechanically rolled EN 10225 Sheet -
Poisson's ratio - Poisson's ratio of 0.3 [-] - - - Typical for Steel
Reduction of area - Reduction of area of 39.8 % - - - Predicted Value
- - Reduction of area of 44.4 % - - - Predicted Value, Transverse
Shear modulus - Shear modulus of 79.9 GPa - - - Predicted Value
Shear strength - Shear strength of 544.9 MPa - - - Predicted Value
Tensile strength 20 °C Tensile strength of 500 - 700 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 500 - 690 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 500 - 680 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 500 - 675 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 500 - 665 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 500 - 660 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 505 - 700 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 505 - 690 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 505 - 680 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 505 - 675 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 505 - 665 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 505 - 660 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 515 - 700 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 515 - 690 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 515 - 680 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 515 - 675 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 515 - 665 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 515 - 660 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 520 - 700 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 520 - 690 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 520 - 680 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 520 - 675 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 520 - 665 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 520 - 660 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 530 - 700 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 530 - 690 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 530 - 680 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 530 - 675 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 530 - 665 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 530 - 660 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 540 - 700 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 540 - 690 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 540 - 680 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 540 - 675 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 540 - 665 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Tensile strength of 540 - 660 MPa thermomechanically rolled EN 10225 Sheet -
Yield strength - Yield strength of 263.4 MPa - - - Predicted Value, RP1
- - Yield strength of 318.6 MPa - - - Predicted Value, RP1 Transverse
- - Yield strength of 425.5 MPa - - - Predicted Value, RP02
- - Yield strength of 431.2 MPa - - - Predicted Value, Transverse
- - Yield strength of 487.7 MPa - - - Predicted Value, RP02 Transverse
- - Yield strength of 500.1 MPa - - - Predicted Value, RP05
- - Yield strength of 528 MPa - - - Predicted Value, RP002
- 20 °C Yield strength of 400 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Yield strength of 405 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Yield strength of 415 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Yield strength of 420 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Yield strength of 440 MPa thermomechanically rolled EN 10225 Sheet -
- 20 °C Yield strength of 460 MPa thermomechanically rolled EN 10225 Sheet -