EN 10225 Grade S420G2 thermomechanically rolled

EN 10225 Grade S420G2 thermomechanically rolled introduction

The standard is applicable to steels for offshore structures, designed to operate in the offshore sector but not to steels supplied for the fabrication of subsea pipelines, risers, process equipment, process piping, and other utilities. It is primarily applicable to the North Sea Sector, but may also be applicable in other areas provided that due consideration is given to local conditions e.g. temperature.

Equivalent material: EN S420G2+M, DIN 1.8857, DIN S420G2, EN 1.8857

EN 10225 Grade S420G2 thermomechanically rolled general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 g/cm³ Typical for Steel

EN 10225 Grade S420G2 thermomechanically rolled chemical

Property Value
Aluminium Aluminium of 0.015 - 0.055 %
Antimony Antimony of 0.01 %
Arsenic Arsenic of 0.03 %
Bismuth Bismuth of 0.01 %
Boron Boron of 1E-3 %
Calcium Calcium of 5E-3 %
Carbon Carbon of 0.14 %
Chromium Chromium of 0.25 %
Copper Copper of 0.3 %
Lead Lead of 0.01 %
Manganese Manganese of 1.65 %
Molybdenum Molybdenum of 0.25 %
Nickel Nickel of 0.7 %
Niobium Niobium of 0.04 %
Nitrogen Nitrogen of 0.01 %
Phosphorus Phosphorus of 0.02 %
Silicon Silicon of 0.15 - 0.55 %
Sulfur Sulfur of 7E-3 %
Tin Tin of 0.02 %
Titanium Titanium of 0.03 %
Vanadium Vanadium of 0.08 %

EN 10225 Grade S420G2 thermomechanically rolled mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 190 - 210 GPa Typical for Steel
Elongation 20.0 °C Elongation of 19 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Steel
Tensile strength 20.0 °C Tensile strength of 480 - 660 MPa -
Yield strength 20.0 °C Yield strength of 380 - 420 MPa -