EN 10213 Grade G18Mo5 quenched and tempered (+QT)

EN 10213 Grade G18Mo5 quenched and tempered (+QT) introduction

Tough at low temperature steel casting for pressure purposes.

Equivalent material: ISO G18Mo5, DIN 1.5422, EN 1.5422, UNS J12522

EN 10213 Grade G18Mo5 quenched and tempered (+QT) general

Property Temperature Value
Density 20.0 °C Density of 7.85 g/cm³

EN 10213 Grade G18Mo5 quenched and tempered (+QT) thermal

Property Temperature Value Comment
Coefficient of thermal expansion 100.0 °C Coefficient of thermal expansion of 1.24E-5 1/K -
- 300.0 °C Coefficient of thermal expansion of 1.31E-5 1/K -
- 500.0 °C Coefficient of thermal expansion of 1.38E-5 1/K -
Max service temperature, long - Max service temperature, long of -45 - 0 °C -
Melting point - Melting point of 1382 - 1529 °C Typical for Molybdenum Steel
Specific heat capacity 20.0 °C Specific heat capacity of 460 J/(kg·K) -
Thermal conductivity 50.0 °C Thermal conductivity of 43 W/(m·K) -

EN 10213 Grade G18Mo5 quenched and tempered (+QT) chemical

Property Value
Carbon Carbon of 0.15 - 0.2 %
Chromium Chromium of 0.3 %
Copper Copper of 0.3 %
Manganese Manganese of 0.8 - 1.2 %
Molybdenum Molybdenum of 0.45 - 0.65 %
Nickel Nickel of 0.4 %
Phosphorus Phosphorus of 0.02 %
Silicon Silicon of 0.6 %
Sulfur Sulfur of 0.02 %
Vanadium Vanadium of 0.05 %

EN 10213 Grade G18Mo5 quenched and tempered (+QT) mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Molybdenum Steel
Elongation 20.0 °C Elongation of 23 % -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Molybdenum Steel
Tensile strength 20.0 °C Tensile strength of 440 - 790 MPa -
Yield strength Rp0.2 20.0 °C Yield strength Rp0.2 of 240 MPa -