EN 10209 Grade DC06ED cold rolled, skin passed

EN 10209 Grade DC06ED cold rolled, skin passed introduction

Cold rolled low carbon steel for flat products for vitreous enamelling (direct enamelling, as well as for special applications of conventional two coat enamelling for better sag resistance).
Application: domestic appliances (cooking, laundry), sanitary ware (bathtubs, shower trays, sinks), architectural panels (interior and exterior), signage

Equivalent material: ASTM A424Type, DIN 1.0872, DIN FeD 6, DIN DC06ED, AFNOR DC06ED, BS DC06ED, EN 1.0872

EN 10209 Grade DC06ED cold rolled, skin passed general

Property Value Comment
Density Density of 7.8 - 7.9 g/cm³ Typical for Low Carbon Steel

EN 10209 Grade DC06ED cold rolled, skin passed thermal

Property Value Comment
Coefficient of thermal expansion Coefficient of thermal expansion of 1.32e-05 - 1.38e-05 1/K Typical for Low Carbon Steel
Max service temperature Max service temperature of 500 °C Typical for Carbon Steel
Melting point Melting point of 1480 - 1526 °C Typical for Low Carbon Steel
Specific heat capacity Specific heat capacity of 465 J/(kg·K) Typical for Low Carbon Steel
Thermal conductivity Thermal conductivity of 25 - 93 W/(m·K) Typical for Low Carbon Steel

EN 10209 Grade DC06ED cold rolled, skin passed chemical

Property Value Condition Related Standards Shape
Carbon Carbon of 0.02 cold rolled, skin passed EN 10209 Sheet
Manganese Manganese of 0.35 cold rolled, skin passed EN 10209 Sheet
Phosphorus Phosphorus of 0.02 cold rolled, skin passed EN 10209 Sheet
Sulfur Sulfur of 0.05 cold rolled, skin passed EN 10209 Sheet
Titanium Titanium of 0.3 cold rolled, skin passed EN 10209 Sheet

EN 10209 Grade DC06ED cold rolled, skin passed magnetic

Property Value Comment
Curie temperature Curie temperature of 770 °C Typical for Low Carbon Steel

EN 10209 Grade DC06ED cold rolled, skin passed electrical

Property Value Comment
Electrical resistivity Electrical resistivity of 1.43e-07 - 1.74e-07 Ω·m Typical for Carbon Steel

EN 10209 Grade DC06ED cold rolled, skin passed mechanical

Property Temperature Value Condition Related Standards Shape Comment
Elastic modulus - Elastic modulus of 200 - 215 GPa - - - Typical for Low Carbon Steel
Poisson's ratio - Poisson's ratio of 0.29 [-] - - - Typical for Low Carbon Steel
Shear modulus - Shear modulus of 82 GPa - - - Typical for Low Carbon Steel
Tensile strength 20 °C Tensile strength of 270 - 350 MPa cold rolled, skin passed EN 10209 Sheet Transverse
- 20 °C Tensile strength of 270 - 350 MPa cold rolled, skin passed EN 10209 Strip, Bar -
Yield strength 20 °C Yield strength of 120 - 230 MPa cold rolled, skin passed EN 10209 Sheet Transverse
- 20 °C Yield strength of 120 - 210 MPa cold rolled, skin passed EN 10209 Sheet Transverse
- 20 °C Yield strength of 120 - 190 MPa cold rolled, skin passed EN 10209 Sheet Transverse
- 20 °C Yield strength of 120 - 190 MPa cold rolled, skin passed EN 10209 Strip, Bar -

From fabrication to delivery, we ensure excellence in every aspect of our steel products.

-- Our promise