EN 10209 Grade DC04ED cold rolled, skin passed
EN 10209 Grade DC04ED cold rolled, skin passed introduction
Cold rolled low carbon steel for flat products for vitreous enamelling (direct enamelling, as well as for special applications of conventional two coat enamelling for better sag resistance).
Application: domestic appliances (cooking, laundry), sanitary ware (bathtubs, shower trays, sinks), architectural panels (interior and exterior), signage
Equivalent material: DIN ED4, DIN 1.0394, DIN ED 4, DIN DC04ED, AFNOR DC04ED, BS DC04ED, EN 1.0394
EN 10209 Grade DC04ED cold rolled, skin passed general
Property |
Value |
Comment |
Density |
Density of 7.8 - 7.9 g/cm³ |
Typical for Low Carbon Steel |
EN 10209 Grade DC04ED cold rolled, skin passed thermal
Property |
Value |
Comment |
Coefficient of thermal expansion |
Coefficient of thermal expansion of 1.32e-05 - 1.38e-05 1/K |
Typical for Low Carbon Steel |
Max service temperature |
Max service temperature of 500 °C |
Typical for Carbon Steel |
Melting point |
Melting point of 1480 - 1526 °C |
Typical for Low Carbon Steel |
Specific heat capacity |
Specific heat capacity of 465 J/(kg·K) |
Typical for Low Carbon Steel |
Thermal conductivity |
Thermal conductivity of 25 - 93 W/(m·K) |
Typical for Low Carbon Steel |
EN 10209 Grade DC04ED cold rolled, skin passed chemical
Property |
Value |
Condition |
Related Standards |
Shape |
Carbon |
Carbon of 0.004 |
cold rolled, skin passed |
EN 10209 |
Sheet |
Manganese |
Manganese of 0.4 |
cold rolled, skin passed |
EN 10209 |
Sheet |
Phosphorus |
Phosphorus of 0.03 |
cold rolled, skin passed |
EN 10209 |
Sheet |
Sulfur |
Sulfur of 0.05 |
cold rolled, skin passed |
EN 10209 |
Sheet |
EN 10209 Grade DC04ED cold rolled, skin passed magnetic
Property |
Value |
Comment |
Curie temperature |
Curie temperature of 770 °C |
Typical for Low Carbon Steel |
EN 10209 Grade DC04ED cold rolled, skin passed electrical
Property |
Value |
Comment |
Electrical resistivity |
Electrical resistivity of 1.43e-07 - 1.74e-07 Ω·m |
Typical for Carbon Steel |
EN 10209 Grade DC04ED cold rolled, skin passed mechanical
Property |
Temperature |
Value |
Condition |
Related Standards |
Shape |
Comment |
Elastic modulus |
- |
Elastic modulus of 200 - 215 GPa |
- |
- |
- |
Typical for Low Carbon Steel |
Poisson's ratio |
- |
Poisson's ratio of 0.29 [-] |
- |
- |
- |
Typical for Low Carbon Steel |
Shear modulus |
- |
Shear modulus of 82 GPa |
- |
- |
- |
Typical for Low Carbon Steel |
Tensile strength |
20 °C |
Tensile strength of 270 - 350 MPa |
cold rolled, skin passed |
EN 10209 |
Sheet |
Transverse |
- |
20 °C |
Tensile strength of 270 - 350 MPa |
cold rolled, skin passed |
EN 10209 |
Strip, Bar |
- |
Yield strength |
20 °C |
Yield strength of 140 - 260 MPa |
cold rolled, skin passed |
EN 10209 |
Sheet |
Transverse |
- |
20 °C |
Yield strength of 140 - 230 MPa |
cold rolled, skin passed |
EN 10209 |
Sheet |
Transverse |
- |
20 °C |
Yield strength of 140 - 210 MPa |
cold rolled, skin passed |
EN 10209 |
Sheet |
Transverse |
- |
20 °C |
Yield strength of 140 - 225 MPa |
cold rolled, skin passed |
EN 10209 |
Sheet |
Transverse |
- |
20 °C |
Yield strength of 140 - 210 MPa |