EN 10203 Grade TH415 cold rolled
EN 10203 Grade TH415 cold rolled introduction
TH 415 is a single cold rolled band (black plate in coils) of soft unalloyed steel and in the surface qualities plain, stone finish and matt for conventional packaging sheet. The band is produced in thicknesses of 0,17 to 0,49 mm in steps of 0,005 mm. The surface is oiled in order to avoid corrosion.
The strip is applicated for the production of
- electrolytically tinned tinplate
Tin used for coating has to show a purity grade of 99,85%.
Preferred tin plating values (double-sided) are: 1,0
1,4
2,0
2,8
4,0
5,0
5,6
8,4
11,2
14,0
15,1 g/m²
Tinplate is also delivered diferentially coated. In this case is necessary a special designation .
Appearance of the tinplate surface is determined by the surface characteristics of the basic material and type of tincoating.
Available surface qualities: bright, stone finish, silver matt and matt
- electrolytically special chromed steel (ECCS)
Total Cr-content used for coating consists of metallic chromium and chromium oxides. The mean coating weight of metallic chromium accounts for 50 to 140 mg/m² and 7 to 35 mg/m² for chromium oxides.
Surface appearance of ECCS which follows from the application of work rolls of a special surface texture during the last cold rerolling steps is determined by the surface characteristics of the basic material.
Available surface qualities: matt, plain, stone finish
For the choice of surface refined extra-fine sheets has to be considered the final consumption purpose, e.g. requirements, such as suitability for punching, drawing, folding, beading, welding and soldering.
Application of extra-fine sheets:
- cans, jugs, canister, buckets
- household articles, boxes, closures
- ceiling elements, fittings, pressure plates etc.
Equivalent material: IS TH61+CE, ASTM A657TypeT4, DIN 1.0377, DIN T61, DIN TH61, DIN T 61, DIN TH415, JIS SWCH35K, EN TH61, EN 1.0377
EN 10203 Grade TH415 cold rolled general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 - 7.9 g/cm³ |
Typical for Low Carbon Steel |
EN 10203 Grade TH415 cold rolled thermal
Property |
Temperature |
Value |
Comment |
Coefficient of thermal expansion |
23.0 °C |
Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K |
Typical for Low Carbon Steel |
Max service temperature |
- |
Max service temperature of 500 °C |
Typical for Carbon Steel |
Melting point |
- |
Melting point of 1480 - 1526 °C |
Typical for Low Carbon Steel |
Specific heat capacity |
23.0 °C |
Specific heat capacity of 465 J/(kg·K) |
Typical for Low Carbon Steel |
Thermal conductivity |
23.0 °C |
Thermal conductivity of 25 - 93 W/(m·K) |
Typical for Low Carbon Steel |
EN 10203 Grade TH415 cold rolled magnetic
Property |
Value |
Comment |
Curie temperature |
Curie temperature of 770 °C |
Typical for Low Carbon Steel |
EN 10203 Grade TH415 cold rolled electrical
Property |
Temperature |
Value |
Comment |
Electrical resistivity |
23.0 °C |
Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m |
Typical for Carbon Steel |
EN 10203 Grade TH415 cold rolled mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 200 - 215 GPa |
Typical for Low Carbon Steel |
Hardness, Rockwell T |
20.0 °C |
Hardness, Rockwell T of 60 - 62 [-] |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.29 [-] |
Typical for Low Carbon Steel |
Shear modulus |
23.0 °C |
Shear modulus of 82 GPa |
Typical for Low Carbon Steel |
Tensile strength |
20.0 °C |
Tensile strength of 435 MPa |
- |
Yield strength Rp0.2 |
20.0 °C |
Yield strength Rp0.2 of 415 MPa |
- |
Create sustainable legacies with our eco-friendly steel materials and practices.
-- Our promise
Similar or equivalent steel materials