EN 10202 Grade T660 double reduced

EN 10202 Grade T660 double reduced introduction

TH 660, mat. No 1.0376, is a double cold reduced band (black plate in coils) of soft unalloyed steel and in the surface qualities plain, stone finish and matt for conventional packaging sheet, hardness HR30T m 77. The band is produced in thicknesses of 0,17 to 0,29 mm in steps of 0,005 mm. The surface is oiled in order to avoid corrosion. The band is applicated for the production of
- electrolytically tinned tinplate, DIN EN 10203
Tin used for coating has to show a purity grade of 99,85%.
Preferred tin plating values (double-sided) are:
1,0
1,5
2,0
2,8
4,0
5,0
5,6
8,4
11,2 g/m²
Tinplate is also delivered diferentially coated. In this case is necessary a special designation . Surface appearance of tinplate is determined by the surface characteristics of the basic material and the type of tincoating.
Available surface qualities:
stone finish
- electrolytically special chromed steel (ECCS), DIN EN 10202
Total Cr-content used for coating consists of metallic chromium and chromium oxides. The mean coating weight of metallic chromium accounts for 50 to 140 mg/m² and 7 to 35 mg/m² for chromium oxides.
Surface appearance of ECCS which follows from the application of work rolls of a special surface texture during the last cold rerolling steps is determined by the surface characteristics of the basic material.
Available surface qualities:
stone finish
For the choice of surface refined extra-fine blooms has to be considered the final consumption purpose, e.g. requirements, such as suitability for punching, drawing, folding, beading, welding and soldering.
Application of black plate:
- cans, jugs, canister, buckets
- household articles, boxes, closures
- ceiling elements, fittings, pressure plates etc.

Equivalent material: DIN 1.0376, EN 1.0376

EN 10202 Grade T660 double reduced general

Property Temperature Value Comment
Density 23.0 °C Density of 7.8 - 7.9 g/cm³ Typical for Low Carbon Steel

EN 10202 Grade T660 double reduced thermal

Property Temperature Value Comment
Coefficient of thermal expansion 23.0 °C Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K Typical for Low Carbon Steel
Max service temperature - Max service temperature of 500 °C Typical for Carbon Steel
Melting point - Melting point of 1480 - 1526 °C Typical for Low Carbon Steel
Specific heat capacity 23.0 °C Specific heat capacity of 465 J/(kg·K) Typical for Low Carbon Steel
Thermal conductivity 23.0 °C Thermal conductivity of 25 - 93 W/(m·K) Typical for Low Carbon Steel

EN 10202 Grade T660 double reduced magnetic

Property Value Comment
Curie temperature Curie temperature of 770 °C Typical for Low Carbon Steel

EN 10202 Grade T660 double reduced electrical

Property Temperature Value Comment
Electrical resistivity 23.0 °C Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m Typical for Carbon Steel

EN 10202 Grade T660 double reduced mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 200 - 215 GPa Typical for Low Carbon Steel
Hardness, Rockwell T 20.0 °C Hardness, Rockwell T of 77 [-] -
Poisson's ratio 23.0 °C Poisson's ratio of 0.29 [-] Typical for Low Carbon Steel
Shear modulus 23.0 °C Shear modulus of 82 GPa Typical for Low Carbon Steel
Yield strength Rp0.2 20.0 °C Yield strength Rp0.2 of 660 MPa -