EN 10084 Grade 10NiCr5-4 treated for cold shearing (+S)
Equivalent material: DIN 1.5805, EN 1.5805
EN 10084 Grade 10NiCr5-4 treated for cold shearing (+S) general
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Density | 23.0 °C | Density of 7.8 g/cm³ | Typical for Steel |
EN 10084 Grade 10NiCr5-4 treated for cold shearing (+S) chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.07 - 0.12 % |
| Chromium | Chromium of 0.9 - 1.2 % |
| Manganese | Manganese of 0.6 - 0.9 % |
| Nickel | Nickel of 1.2 - 1.5 % |
| Phosphorus | Phosphorus of 0.04 % |
| Silicon | Silicon of 0.4 % |
| Sulfur | Sulfur of 0.035 % |
EN 10084 Grade 10NiCr5-4 treated for cold shearing (+S) mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
| Elastic modulus | 23.0 °C | Elastic modulus of 190 - 210 GPa | Typical for Steel |
| Poisson's ratio | 23.0 °C | Poisson's ratio of 0.3 [-] | Typical for Steel |