DIN 43720 Grade X10NiCr32-20 quenched (+Q)

DIN 43720 Grade X10NiCr32-20 quenched (+Q) introduction

Heat resistance in air: up to 1200 °C.
Application:
tubes in the petroleum industry

Equivalent material: DIN 1.4861, EN X10NiCr32-20, EN 1.4861

DIN 43720 Grade X10NiCr32-20 quenched (+Q) general

Property Temperature Value
Density 20.0 °C Density of 7.9 g/cm³

DIN 43720 Grade X10NiCr32-20 quenched (+Q) thermal

Property Temperature Value
Coefficient of thermal expansion 400.0 °C Coefficient of thermal expansion of 1.6E-5 1/K
- 800.0 °C Coefficient of thermal expansion of 1.75E-5 1/K
- 1000.0 °C Coefficient of thermal expansion of 1.85E-5 1/K
Specific heat capacity 20.0 °C Specific heat capacity of 500 J/(kg·K)
Thermal conductivity 20.0 °C Thermal conductivity of 12 W/(m·K)

DIN 43720 Grade X10NiCr32-20 quenched (+Q) chemical

Property Value
Carbon Carbon of 0.12 %
Chromium Chromium of 19 - 22 %
Manganese Manganese of 1.5 %
Nickel Nickel of 30 - 34 %
Phosphorus Phosphorus of 0.05 %
Silicon Silicon of 1 %
Sulfur Sulfur of 0.03 %

DIN 43720 Grade X10NiCr32-20 quenched (+Q) electrical

Property Temperature Value
Electrical resistivity 20.0 °C Electrical resistivity of 1.04E-6 Ω·m

DIN 43720 Grade X10NiCr32-20 quenched (+Q) mechanical

Property Temperature Value Comment
Elastic modulus 23.0 °C Elastic modulus of 190 - 210 GPa Typical for Steel
Elongation 20.0 °C Elongation of 30 % -
Hardness, Brinell 20.0 °C Hardness, Brinell of 200 [-] -
Poisson's ratio 23.0 °C Poisson's ratio of 0.3 [-] Typical for Steel
Tensile strength 20.0 °C Tensile strength of 490 - 740 MPa -
Yield strength Rp0.2 20.0 °C Yield strength Rp0.2 of 235 MPa -