DIN 17745 Grade NiCo29-18 soft annealed (+A)
DIN 17745 Grade NiCo29-18 soft annealed (+A) introduction
Application: melting down in hard glass, glass/ceramic metal joints
DIN 17745 Grade NiCo29-18 soft annealed (+A) general
| Property | Temperature | Value |
|---|---|---|
| Density | 20.0 °C | Density of 8.2 g/cm³ |
DIN 17745 Grade NiCo29-18 soft annealed (+A) thermal
| Property | Temperature | Value |
|---|---|---|
| Coefficient of thermal expansion | 100.0 °C | Coefficient of thermal expansion of 6.5E-6 1/K |
| - | 150.0 °C | Coefficient of thermal expansion of 6.2E-6 1/K |
| - | 200.0 °C | Coefficient of thermal expansion of 5.9E-6 1/K |
| - | 300.0 °C | Coefficient of thermal expansion of 5.4E-6 1/K |
| - | 400.0 °C | Coefficient of thermal expansion of 5.1E-6 1/K |
| - | 500.0 °C | Coefficient of thermal expansion of 6.2E-6 1/K |
| - | 600.0 °C | Coefficient of thermal expansion of 7.8E-6 1/K |
| Thermal conductivity | 20.0 °C | Thermal conductivity of 17 W/(m·K) |
DIN 17745 Grade NiCo29-18 soft annealed (+A) chemical
| Property | Value |
|---|---|
| Carbon | Carbon of 0.05 % |
| Cobalt | Cobalt of 16 - 18 % |
| Manganese | Manganese of 0.5 % |
| Nickel | Nickel of 28 - 30 % |
| Silicon | Silicon of 0.3 % |
DIN 17745 Grade NiCo29-18 soft annealed (+A) electrical
| Property | Temperature | Value |
|---|---|---|
| Electrical resistivity | 20.0 °C | Electrical resistivity of 4.5E-7 Ω·m |
DIN 17745 Grade NiCo29-18 soft annealed (+A) mechanical
| Property | Temperature | Value |
|---|---|---|
| Elastic modulus | 20.0 °C | Elastic modulus of 157 GPa |