DIN 17205 Grade GS-35CrMoV10-4 quenched in a liquid medium and tempered, strength grade I

DIN 17205 Grade GS-35CrMoV10-4 quenched in a liquid medium and tempered, strength grade I introduction

The material GS-35 CrMoV 10 4 is applicable up to 300 degrees C, in, among other things, the vehicle manufacturing. The cast material is wear-resistant.

Equivalent material: DIN 1.7755, DIN GS-45CrMoV104, DIN G45CrMoV104, EN G45CrMoV104, EN 1.7755

DIN 17205 Grade GS-35CrMoV10-4 quenched in a liquid medium and tempered, strength grade I general

Property Temperature Value
Density 20.0 °C Density of 7.85 g/cm³

DIN 17205 Grade GS-35CrMoV10-4 quenched in a liquid medium and tempered, strength grade I thermal

Property Temperature Value
Coefficient of thermal expansion 100.0 °C Coefficient of thermal expansion of 1.1E-5 1/K
- 200.0 °C Coefficient of thermal expansion of 1.2E-5 1/K
- 300.0 °C Coefficient of thermal expansion of 1.3E-5 1/K
Max service temperature, long - Max service temperature, long of 0 - 300 °C

DIN 17205 Grade GS-35CrMoV10-4 quenched in a liquid medium and tempered, strength grade I chemical

Property Value
Carbon Carbon of 0.32 - 0.39 %
Chromium Chromium of 2.2 - 2.7 %
Manganese Manganese of 0.6 - 1 %
Molybdenum Molybdenum of 0.3 - 0.5 %
Phosphorus Phosphorus of 0.02 %
Silicon Silicon of 0.6 %
Sulfur Sulfur of 0.015 %
Vanadium Vanadium of 0.05 - 0.15 %

DIN 17205 Grade GS-35CrMoV10-4 quenched in a liquid medium and tempered, strength grade I mechanical

Property Temperature Value
Elastic modulus 20.0 °C Elastic modulus of 211 GPa
- 100.0 °C Elastic modulus of 204 GPa
- 200.0 °C Elastic modulus of 196 GPa
- 300.0 °C Elastic modulus of 186 GPa
Elongation 20.0 °C Elongation of 10 - 15 %
Tensile strength 20.0 °C Tensile strength of 750 - 1000 MPa
Yield strength Rp0.2 20.0 °C Yield strength Rp0.2 of 600 - 700 MPa

Trust our expertise to deliver precision-engineered steel solutions for your specific needs.