DIN 17172 Grade StE385.7 TM thermomechanically treated
DIN 17172 Grade StE385.7 TM thermomechanically treated introduction
The steel StE 385.7 TM is produced as welded tube in the conditions thermomechanical treated.
Tubes of this steel are conform acc. 5L, 5LX and 5LS of the American Petroleum Institute (API). The Attention should be paid to the technical regulation for combustible liquids TRbF 301.
Application:
pipelines for combustible liquids (e.g. petroleum and his products) and for compressed or liquid combustible gases
Equivalent material: DIN 1.8971, EN 1.8971
DIN 17172 Grade StE385.7 TM thermomechanically treated general
Property |
Temperature |
Value |
Comment |
Density |
23.0 °C |
Density of 7.8 g/cm³ |
Typical for Steel |
DIN 17172 Grade StE385.7 TM thermomechanically treated chemical
Property |
Value |
Carbon |
Carbon of 0.14 % |
Manganese |
Manganese of 1 - 1.6 % |
Phosphorus |
Phosphorus of 0.04 % |
Silicon |
Silicon of 0.45 % |
Sulfur |
Sulfur of 0.025 % |
DIN 17172 Grade StE385.7 TM thermomechanically treated mechanical
Property |
Temperature |
Value |
Comment |
Elastic modulus |
23.0 °C |
Elastic modulus of 190 - 210 GPa |
Typical for Steel |
Elongation, transverse |
20.0 °C |
Elongation, transverse of 19 % |
- |
Poisson's ratio |
23.0 °C |
Poisson's ratio of 0.3 [-] |
Typical for Steel |
Tensile strength |
20.0 °C |
Tensile strength of 530 - 680 MPa |
- |
Tensile strength, transverse |
20.0 °C |
Tensile strength, transverse of 530 - 680 MPa |
- |
Yield strength |
20.0 °C |
Yield strength of 385 MPa |
- |
Yield strength, transverse |
20.0 °C |
Yield strength, transverse of 385 MPa |
- |